AWS A5.5 E8016-B8 Welding Electrodes Haʻahaʻa Alloy Steel Weld Rods Stick Arc Weld Materials

ʻO ka wehewehe pōkole:

E8016-B8 Welding Electrodes: Welding of 9% Cr-1% Mo steels a me 9% Cr - 2% Mo steels i hoʻohanaʻia no ka mana uila a me ka moku kiʻekiʻe.


Huahana Huahana

Huahana Huahana

NĀ PALAPALA:

Welding o 9% Cr-1% Mo kila a me 9% Cr - 2% Mo kila i hoʻohana 'ia no ka uila mana a me kiʻekiʻe puʻe moku.

NĀ HOʻOAKAʻI:

PA-8016-B8 mea he haʻahaʻa hydrogen electrode nona weld metala i loko o 9%Cr-1% Mo.Hoʻolālā ʻia ia no ke kila wela a me nā kila no nā lawelawe hydrogen wela, ʻoi loa i ka ʻoihana petrochemical.Hiki ke ʻae ʻia ka electrode no kona ikaika tensile kiʻekiʻe, paʻakikī maikaʻi a me ke kūpaʻa wela nui.

NĀ MANAʻO NO KA HOʻohana:

1. E hoʻomaloʻo i nā electrodes ma 350-400 ° C no hoʻokahi hola ma mua o ka hoʻohana ʻana a mālama i nā electrodes ma 100-150 ° C ma hope o ka hoʻomaloʻo ʻana iā lākou me ka nānā ʻana e pale i ka makū.

2. E hoʻohana i ke ʻano hoʻi i hope a i ʻole e hahau i ke arc ma luna o kahi pā kila liʻiliʻi i hoʻomākaukau ʻia no kēia kumu i mea e pale aku ai i nā pū i ka hoʻomaka ʻana.

3. E mālama i ke arc i ka pōkole e like me ka hiki.

4. E hoʻomoʻa mua i ka 100-150 ° C.ʻOkoʻa ka mahana e hoʻopili ʻia e like me ka mānoanoa pā a me ke ʻano o ke kila e welded.

5. E makaʻala ʻaʻole e ʻoi aku ma mua o ka hoʻokomo wela kūpono no ka mea ʻoi aku ka nui o ka wela-hoʻokomo ʻana ke kumu i ka emi ʻana o nā waiwai hopena a me ka ikaika o ka hoʻoulu ʻana o ka metala weld.

IV.KA HANA KIMAKA MAU O KA WELD METAL (%):

C

Si

Mn

Cr

Mo

0.06

0.42

0.68

9.38

1.05

V. NA WAIWAI MECHANICAL MA'A O WELD METAL:

N/mm2(Ksi)

Lae Hua N/mm2

(Ksi)

Elongation %

PWHT

705 (102)

560 (81)

24

740°C x 1 hola

VI.NA KULANA WELDING: NA KULANA A PAU

VII.KA NUI A ME KA PALAPALA I KEIA NEI (AC/DC+):

Anawaena (mm)

2.5

3.2

4.0

5.0

Ka lōʻihi (mm)

350

350

400

400

Ampere

Palahalaha

55 - 85

90 - 130

130 - 180

180 - 240

V & OH

50 - 80

80 - 115

110 - 170

150 - 200