Laau wiliwili AWS A5.11 ENiCrFe-3 Nā ʻElectrodes wiliwili i hoʻokumu ʻia i ka nikela, nā koʻokoʻo wiliwili nikela.

ʻO ka wehewehe pōkole:

ʻO Ni307-3 (AWS ENiCrFe-3) kahi mea nickel-based electrode me ka haʻahaʻa-hydrogen sodium coating.E hoʻohana i ka DCEP (direct current electrode positive).


Huahana Huahana

Huahana Huahana

Nickel and Nickel Alloy Welding Electrode

Ni307-3                                                     

GB/T ENi6182

AWS A5.11 ENiCrFe-3

ʻO ka wehewehe: Ni307-3 kahinikela-hoʻokumu i ka electrode me ka haʻahaʻa-hydrogen sodium coating.E hoʻohana i ka DCEP (direct current electrode positive).Loaʻa iā ia ke kūpaʻa māwae maikaʻi no ka mea aia i loko o ka weld kekahi nui o ka manganese, niobium, a me nā mea hoʻohui ʻē aʻe.

Hoʻohana: Hoʻohana ʻia ia no ka wili ʻana onikela- chromium-iron alloys (e like me UNS N06600) a me ka ihu o ke kila.ʻAʻole ʻoi aku ka kiʻekiʻe o ka mahana hana ma mua o 480 ° C, a ʻoi aku ka maikaʻi o ka pale ʻana.He kūpono no ka moku ʻumeke umu atomika a me ka wiliwili pahu kemika.

 

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Fe

P

S

Si

Cu

≤0.10

5.0 ~ 10.0

≤10.0

≤0.020

≤0.015

≤1.0

≤0.5

Ni

Ti

Mo

Nb

Ta

'ē aʻe

 

≥60.0

≤1.0

13.0 ~ 17.0

1.0 ~ 3.5

≤0.30

≤0.50

 

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

Hua ikaika

Mpa

ʻO ka lōʻihi

%

Hōʻoiaʻiʻo

≥550

≥360

≥27

 

Manaʻo ʻia i kēia manawa:

Anawaena lāʻau

(mm)

2.5

3.2

4.0

5.0

Ke au wiliwili

(A)

60 ~ 90

80 ~ 100

110 ~ 150

130 ~ 180

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 300 ℃ ma mua o ka hana wili;

2. Pono pono e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila, ka wai, a me nā haumia ma nā ʻāpana wili ma mua o ka wili ʻana.E ho'āʻo e hoʻohana i kahi pōkā pōkole e wili.

 