ʻO ka wehewehe pōkole:

AWS A5.1 E7015 mea haʻahaʻa-hydrogen sodium uhi carbon kila electrode.


Huahana Huahana

Huahana Huahana

AWS A5.1 E7015 mea haʻahaʻa-hydrogen sodium uhi carbon kila electrode.

Pono e hoʻohana ʻia ka E7015 welding electrode ma DCEP.Loaʻa iā ia ka hoʻohana wili maikaʻi loa e hiki ai iā ia ke hana i nā kūlana āpau, he paʻa arc, maʻalahi ka wehe ʻana i ka slag a he haʻahaʻa haʻahaʻa.ʻO ka metala i hoʻopaʻa ʻia he hana mechanical maikaʻi a me ke kūpaʻa-kūʻē, e hāʻawi ana i ka ikaika haʻahaʻa haʻahaʻa maikaʻi.

Palapala noi

Hoʻohana ʻia ʻo AWS A5.1 E7015 i ka hoʻoheheʻe ʻana i ke kila medium-carbon a me nā hale haʻahaʻa haʻahaʻa e like me 16Mn, 09Mn2Si, 09Mn2V a me nā kila i hoʻohana ʻia i ka hana moku e like me A, B, D, E. nā hale kila kalapona paʻakikī e wili.

Kūlike me ke Kūlana

GB/T 5117 E5015

AWS A5.1 E7015

ISO 2560-BE 49 15 A

Ke kumu: Hoʻohana ʻia ʻo AWS A5.1 E7015 i ka hoʻopili ʻana i ke kila waena-carbon a me nā hale haʻahaʻa haʻahaʻa e like me 16Mn, 09Mn2Si, 09Mn2V a me nā kila i hoʻohana ʻia i ka hana moku e like me A, B, D, E. Hoʻohana pū ʻia i ke kila mānoanoa nā papa a me nā hale kila kalapona i paʻakikī ke wili.

Huina Kemika(%)

Hoʻohui Kimia

C

Mn

Si

S

P

Ni

Cr

Mo

V

Waiwai Hōʻoia

≤

0.15

≤

1.60

≤

0.90

≤0.035

≤0.035

≤

0.30

≤

0.20

≤

0.30

≤

0.08

Hua nui

0.082

1.10

0.58

0.012

0.021

0.011

0.028

0.007

0.016

Nā Pono Mechanical o ka metala i waiho ʻia (Ke kinoea pale: CO2)

Mea hoao

Rm(MPa)

ReL(MPa)

A(%)

KV2(J)

-20 ℃ -30 ℃

Waiwai Hōʻoia

≥490

≥400

≥20

≥47

≥27

Hua nui

550

450

32

150

142

X-Ray Radio-graphic Koi Hoao: Papa I

Hōʻike i kēia manawa (DC+)

Anawaena(mm)

Φ2.5

Φ3.2

Φ4.0

Φ5.0

Amperage(A)

60~100

80~140

110~210

160~230

Nā memo:

1. Pono e hoʻomaʻamaʻa mua ʻia ka electrode i ka mahana o 350 ° C no 1 hola.E hoʻomehana i ke koʻokoʻo ke hoʻohana ʻia.

2. Pono e hoʻomaʻemaʻe ʻia nā mea haumia e like me ka ʻōpala, ka ʻaila ʻaila a me ka makū mai ka ʻāpana hana.

3. Pono ka pōkole pōkole e hana i ka wili.ʻOi ʻia ke ala weld haiki.