AWS ENiFe-CI (Z408) Maʻemaʻe Nickel hoʻoheheʻe ʻia nā Electrodes

ʻO ka wehewehe pōkole:

He kūpono ia no ka hoʻopili ʻana i ka hao hina ikaika a me ka hao nodular, e like me ka cylinder, block engine, gear box, etc.


Huahana Huahana

Huahana Huahana

NĀ PALAPALA:

He kūpono ia no ka hoʻopili ʻana i ka hao hina ikaika a me ka hao nodular, e like me ka cylinder, block engine, gear box, etc.

NĀ PĀLĀWAI:

AWS A5.15 / ASME SFA5.15 ENiFe-CI

JIS Z3252 DFCNiFe

NA ANOAI:

ʻO AWS ENiFe-CI (Z408) ka mea hao hao me ka nickel iron alloy core a me ka hoʻohaʻahaʻa ikaika o ka uhi graphite.Hiki ke hoʻohana ʻia i ka AC a me DC kumu ʻelua, loaʻa ka arc paʻa, a maʻalahi ke hana.Loaʻa i ka electrode nā hiʻohiʻona o ka ikaika kiʻekiʻe, ka plasticity maikaʻi, ka hoʻonui laina laina haʻahaʻa a pēlā aku.ʻO ka pale ʻana o ka māwae no ka hao hina hina e like me ia no Z308, ʻoiai ʻoi aku ka nui o ka pale ʻana no ka hao nodular ma mua o ENi-CI (Z308).No ka hao hao me ka phosphorus kiʻekiʻe (0.2%P), he hopena maikaʻi nō hoʻi a ʻoi aku ka haʻahaʻa o kāna hana ʻoki ʻana ma mua o Z308 a me Z508.Hoʻohana ʻia ʻo Z408 i ke kuʻi ʻana o ka hao hina a me ka hao nodular no ka lumi

NĀ MEA:

Ma mua o ke kuʻi ʻana, pono e kālua ʻia nā electrodes no 1 hola me ka mahana o 150±10 ℃ ma mua o ka hoʻohana ʻana.

I ka wā e wili ai, pono ia e lawe i ka weld liiki a ʻaʻole pono ka lōʻihi o kēlā me kēia weld ma mua o 50mm.E hoʻomāmā i ka wahi hoʻoheheʻe me ka hāmare ma hope koke o ka wili ʻana i mea e hoʻopau ai i ke kaumaha a pale i nā māwae.

Hoʻokomo ʻia ka wela haʻahaʻa.

KA HANA KIMIKA O KA METAL DEPOSITED(KA MASS FACTION):%

ʻElemu

C

Si

Mn

S

Fe

Ni

Cu

ʻO ka nui o nā mea ʻē aʻe

Waiwai maʻamau

0.35-0.55

≤0.75

≤

2.3

≤0.025

3.0-

6.0

60-

70

25-

35

≤

1.0

WEELDING REFERENCE CURRENT:(AC,DC+)

Anawaena uila (mm)

3.2

4.0

5.0

Ka lōʻihi (mm)

350

350

350

Ke au wiliwili (A)

90-110

120-150

160-190

Nā ʻano ma ka hoʻohana ʻana:

Paʻa loa arc.

Hiki ke hoʻoneʻe maikaʻi ʻia o ka slag.

He pāpaʻu ke komo ʻana.

ʻO ke kūpaʻa wela a me ka corrosion maikaʻi.

Kūleʻa māwae maikaʻi.