ʻO ka wehewehe pōkole:

ʻO A201(AWS E316-16) kahi haʻahaʻa haʻahaʻa Cr18Ni12Mo2 stainless steel electrode me ka titanium-calcium coating.


Huahana Huahana

Huahana Huahana

Electrode wiliwili kila

A201                                      

GB/T E316-16

AWS E316-16

ʻO ka wehewehe: ʻO A201 kahi haʻahaʻa haʻahaʻa Cr18Ni12Mo2 stainless steel electrode me ka titanium-calcium coating.Hiki ke hoʻohana ʻia no ka AC a me DC me ka hana maikaʻi loa, ʻoi aku ka maikaʻi no ka wili paʻa a me ka hoʻopili ʻana i nā papa lahilahi.ʻAʻole ʻulaʻula a māwae paha ka uhi i ka wā wili.Ma muli o ka hoʻohui ʻana o ka molybdenum i ka metala i waiho ʻia, loaʻa iā ia ka pale ʻana i ka corrosion maikaʻi, ka pale ʻana i ka wela a me ka pale ʻana i ka māwae, ʻoi aku ka maikaʻi no ka pale ʻana i ka chloride ion pitting corrosion.

Hoʻohana: Hoʻohana ʻia no ka wiliwili 06Cr17Ni12Mo2 mau hale kila kila e hana ana i loko o ka mea kūlohelohe a me ka inorganic acid (non-oxidizing acid) medium, a hiki ke hoʻohana ʻia no ke kuʻi ʻana i ke kila chromium kiʻekiʻe a i ʻole ke kila like ʻole ʻaʻole hiki ke mālama ʻia i ka wela ma hope o ke kuʻi ʻana.

 

 

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

ʻO ka lōʻihi

%

Hōʻoiaʻiʻo

≥520

≥30

 

Manaʻo ʻia i kēia manawa:

Anawaena lāʻau

(mm)

2.0

2.5

3.2

4.0

5.0

Ke au wiliwili

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 250 ℃ ma mua o ka hana wili.Mai kalua pinepine;

2. No ka mea he pāpaʻu ka hohonu o ke komo ʻana i ka wā o ka hoʻoheheʻe ʻana o AC, pono e hoʻohana ʻia ka mana DC e like me ka hiki ke loaʻa i ka hohonu hohonu.

 

Ua hoʻokumuʻiaʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hanaʻana i nā electrodes wiliwili, nā koʻokoʻo hoʻoheheʻe, a me nā mea hoʻohana no nā makahiki he 20.

ʻO kā mākou huahana nui e pili ana i nā electrodes kuʻekuʻe, carbon steel welding electrodes. alumini wili uwea, submerged arc welding.uea, nickel & cobalt alloy uea, keleawe wiliwili uea, TIG & MIG wiliwili uea, tungsten electrodes, carbon gouging electrodes, a me na mea wiliwili 'ē aʻe a me nā mea hoʻohana.