ʻElekode Kuʻi Paʻakikī a me ke Kūpaʻa ʻo ECoCr-A (Cobalt 6) Cobalt

Wehewehe Pōkole:

Hoʻohana ʻia ʻo A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods no ka hoʻopili ʻana i nā poʻo valve, nā apo sila o ka pamu kaomi kiʻekiʻe a me nā ʻāpana o nā mea wili.


Nā kikoʻī huahana

Nā Lepili Huahana

ʻElekode Kuʻi Paʻakikī a me ke Kūpaʻa ʻo ECoCr-A (Cobalt 6) Cobalt

ʻAno Alloy: A5.13, SOLID SURFACING Nā Electrodes a me nā Rods Welding, A5.13
ʻO ECoCr-A Cobalt Alloy 6 ka mea i hoʻohana nui ʻia o nā mea hoʻohui cobalt kūpaʻa i ke komo ʻana a hōʻike i ka hana maikaʻi a puni. Ua manaʻo ʻia ʻo ia ke kūlana ʻoihana no nā noi pale ʻana i ke komo ʻana ma ke kumu laulā, he kūpaʻa maikaʻi loa i nā ʻano he nui o ka hoʻohaʻahaʻa mechanical a me ke kemika ma luna o kahi ākea ākea o ka mahana, a mālama i kahi pae paʻakikī kūpono a hiki i 500⁰C (930⁰F). Loaʻa iā ia kahi kūpaʻa maikaʻi i ka hopena a me ka cavitation erosion. He kūpono loa ʻo Cobalt Alloy 6 i nā ʻano hana paʻakikī like ʻole a hiki ke hoʻohuli ʻia me nā mea hana carbide.

Nā Hoʻohana Maʻamau: nā pahi ʻokiʻoki; nā kiwikā kahe wai; nā wili extrusion; nā bushings ʻōwili; wela kiʻekiʻe; ʻilikai e hali ana i ka kiwikā

Papa AWS: ECoCr-A Palapala hōʻoia: AWS A5.13/A5.13M:2010
Mea hoʻohuihui: ECoCr-A ASME SFA A5.13

 

Kūlana Kuʻihao:
F, V, OH, H
I kēia manawa:
*NS

 

Ikaika Uila, kpsi: *NS
Ka ikaika o ka hāʻawi ʻana, kpsi: *NS
% Hoʻolōʻihi: *NS

*ʻAʻole i kuhikuhi ʻia ʻo NS

Kemika Uea Maʻamau e like me AWS A5.13 (ʻo nā waiwai hoʻokahi ka palena kiʻekiʻe loa)

C Mn Si Cr Ni Mo Fe W Co ʻĒ aʻe
0.7-1.4 2.0 2.0 25-32 3.0 1.0 5.0 3.0-6.0 Rem 1.0