ENiFe-CI Nickel Alloy Welding Uea, FN 55 Nickel Tig Uea Ferro-nickel Solid Uea

ʻO ka wehewehe pōkole:

ʻO ka uwea paʻa Ferro-nickel i hoʻohana ʻia no ka wili ʻana i ka hao a me ka hao ductile.


Huahana Huahana

Huahana Huahana

ʻAi NikelaUea wiliwili Uea TigENiFe-CI

Nā kūlana
EN ISO 1071 – SC NiFe-1
AWS A5.15 – E NiFe-CI

 

Nā hiʻohiʻona a me nā noi

Fero-nikelauwea paʻa i hoʻohana ʻia no ka wiliwili i ka hao a me ka hao ductile.

He kūpono no nā hui like ʻole ma waena o ka hao hoʻolei, ke kila ʻoluʻolu, ke kila haʻahaʻa a me nā kila kila.

Manaʻo ʻia no ka wiliwili ʻana i ka sulfur kiʻekiʻe, ka phosphorous a i ʻole ka lubricant-contaminated castings.

Hoʻohana maʻamau no ka hoʻoponopono ʻana a me nā noi hana, me ke kūkulu hou ʻana i nā shafts, nā huila, nā hui koʻikoʻi ma waena o ke kila a me ka hao, etc.

Nā mea kumu maʻamau

ʻO ka hao hina hina, ʻoluʻolu, nodular*
* Hoʻohālikelike, ʻaʻole papa inoa piha

 

Huina Kemika %

C%

Mn%

Si%

P%

S%

   

max

max

max

max

max

   

2.00

0.80

0.20

0.03

0.03

   

   

Fe%

Ni%

Cu%

Al%

   

rem.

54.00

max

max

   

56.00

2.50

1.00

   

 

Na Waiwai Mechanical
Ikaika U'i 400 – 579 MPa  
Hua ikaika -  
ʻO ka lōʻihi -  
Ka ikaika o ka hopena -  

ʻOkokoke nā waiwai mīkini a ʻokoʻa paha ma muli o ka wela, ke kinoea pale, nā ʻāpana wili a me nā mea ʻē aʻe.

 

Nā kinoea pale

EN ISO 14175 – TIG: I1 (Argon)

 

Kūlana Welding

EN ISO 6947 – PA, PB, PC, PD, PE, PF

 

ʻIkepili Packaging

Anawaena

Ka lōʻihi

Kaumaha

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

Kuleana: ʻOiai ua hoʻoikaika ʻia nā hana kūpono e hōʻoia i ka pololei o ka ʻike i loaʻa, hiki ke hoʻololi ʻia kēia ʻike me ka ʻole o ka hoʻolaha ʻana a hiki ke noʻonoʻo ʻia he kūpono no ke alakaʻi ākea.

 