ʻO ka wehewehe pōkole:

ʻO Alloy 825 (ERNiFeCr-1) he uwea nickel-iron-chromium e hana ana i kēia koho kūpono no nā ʻano hana paʻakikī.


Huahana Huahana

Huahana Huahana

ʻAi NikelaUea wiliwiliUea TigERNiFeCr-1

Nā kūlana
EN ISO 18274 – Ni 8065 – NiFe30Cr21Mo3
AWS A5.14 – ER NiFeCr-1

 

Nā hiʻohiʻona a me nā noi

ʻO ka huila 825 he anikela-iron-chromium wire e hana ana i kēia koho kūpono no nā ʻano hana paʻakikī.

Hāʻawi kēia uea i nā pae kiʻekiʻe o ka pale ʻana i ka corrosion i nā kaiapuni haʻahaʻa oxidizing a hoʻemi.

Pono no ka uhi uhi ʻana i kahi e makemake ʻia ai ke ʻano kemika like.

ʻOi aku ka maikaʻi loa me ka austenitic weld metala me ke kūpaʻa kiʻekiʻe e kūʻē i ke koʻikoʻi ʻinoʻino i ka pohā i loko o ka media i loaʻa nā ion chloride.

Hoʻohana maʻamau i nā ʻoihana hana kemika, petrochemical, hana pepa a me ka hana mana etc.

 

Nā mea kumu maʻamau

G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, N08904, N08904, ALLOY 802 N. .4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465 , 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586*
* Hoʻohālikelike, ʻaʻole papa inoa piha

 

Huina Kemika %

C%

Mn%

Fe%

P%

S%

Si%

 

max

0.70

22.00

max

max

max

 

0.05

0.90

min

0.020

0.004

0.50

 

 

Cu%

Ni%

Al%

Ti%

Cr%

Mo%

 

2.30

43.00

max

1.00

22.00

3.00

 

3.00

46.00

0.20

1.20

23.50

3.50

 

 

Na Waiwai Mechanical
Ikaika U'i ≥550 MPa  
Hua ikaika -  
ʻO ka lōʻihi -  
Ka ikaika o ka hopena -  

ʻOkokoke nā waiwai mīkini a ʻokoʻa paha ma muli o ka wela, ke kinoea pale, nā ʻāpana wili a me nā mea ʻē aʻe.

 

Nā kinoea pale

EN ISO 14175 – TIG: I1 (Argon)

 

Kūlana Welding

EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG

 

ʻIkepili Packaging
Anawaena Ka lōʻihi Kaumaha  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 