ʻO AWS E317-16 Stainless Steel Welding Rods Arc Welding Stcik Welding Electrodes

Wehewehe Pōkole:

ʻO A242 (AWS E317-16) he electrode kila kila Cr19Ni13Mo3 haʻahaʻa-kalapona me ka uhi titanium-calcium.


Nā kikoʻī huahana

Nā Lepili Huahana

Kuʻihao kila kilaʻElekoda

A242                                      

GB/T E317-16

ʻAWS A5.4 E317-16

Wehewehe: ʻO A242 kahi electrode kila kila Cr19Ni13Mo3 haʻahaʻa-kalapona me ka uhi titanium-calcium. Hiki ke hoʻohana ʻia no AC a me DC me ka hana hana maikaʻi loa. ʻOi aku ka nui o ka molybdenum o ka metala i waiho ʻia ma mua o A202, a ʻoi aku ka maikaʻi o kona kūpaʻa ʻana i ka pala i nā waikawa non-oxidizing, e like me ka sulfuric acid, sulfurous acid, phosphoric acid a me nā waikawa organik. Loaʻa iā ia ka hopena maikaʻi e kūʻē i ka pitting corrosion.

Noi: Hoʻohana ʻia no ka hoʻopili ʻana o nā ʻano kila kila like ʻole a me ke kila hui pū ʻia a me ke kila like ʻole.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

12.0 ~ 14.0

2.0 ~ 4.0

≤0.75

≤0.030

≤0.040

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

Mea hoʻāʻo

Ikaika tensile

Mpa

Hoʻolōʻihi

%

Hōʻoiaʻiʻo ʻia

≥550

≥25

 

Manaʻo ʻia kēia manawa:

Anawaena o ke koʻokoʻo

(mm)

2.5

3.2

4.0

5.0

Au Kuʻihao

(A)

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma 150 ℃ ma mua o ka hana kuʻihao;

2. No ka mea, he papau ka hohonu o ke komo ʻana i ka wā o ka wiliwili AC, pono e hoʻohana ʻia ka mana DC i ka hiki ke komo hohonu. a ʻaʻole pono e nui loa ke au e pale aku ai i ka ʻulaʻula o ke koʻokoʻo wiliwili.

 

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana oʻeleka uila hoʻoheheʻes, nā koʻokoʻo wili, a menā mea hoʻopau kuʻihaono nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me nā electrodes wili kila kila, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili nickel & cobalt alloy, nā uea wili kila māmā & haʻahaʻa alloy, nā uea wili kila kila, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili nickel & cobalt alloy, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 