Mea Hoʻolako Mea Hoʻopau Kuʻi EM14KS Uea Kuʻi Arc Submerged, Nā Koʻokoʻo Kila Kalapona no ka Kuʻi Arc Submerged

Wehewehe Pōkole:

He electrode kila kalapona ʻo EM14KS me ka ʻiʻo hao no ka hoʻoheheʻe ʻana i lalo o ka wai.


Nā kikoʻī huahana

Nā Lepili Huahana

He electrode kila kalapona ʻo EM14KS me ka ʻiʻo hao no ka hoʻoheheʻe ʻana i ka arc i lalo. Ua manaʻo ʻia no ka hoʻoheheʻe ʻana i ke kalapona, a me kekahi mau kila metala haʻahaʻa, ma nā kūlana fillet pālahalaha a me ka pae. Loaʻa i kekahi EM14KS nā hoʻohui liʻiliʻi o ka titanium e hoʻomaikaʻi ana i ka paʻakikī o ka metala hoʻoheheʻe a kōkua i ka mālama ʻana i ka ikaika ma hope o ka hoʻomaha ʻana i ke kaumaha. Pono e hoʻohana ʻia kēia electrode no ka hoʻoheheʻe ʻana i ka arc i lalo wale nō.

KA HOʻOKAʻAWALE ʻANA:

EC1 no AWS A5.17, SFA 5.17.

NĀ ʻANO:

Ua hoʻolālā ʻia ʻo Select EM14KS e hana i kahi kemika waiho weld e like me ka mea i hana ʻia e ka uea paʻa, nā electrodes EM14K. ʻO ka hoʻolālā uea cored e hopena i nā helu waiho kiʻekiʻe ma mua o ka uea paʻa ke holo ʻia ma ka pae au like.

ʻOi aku ka laulā o ke komo ʻana o ka bead ma o ke koho ʻana i ka EM14KS ma mua o ke kaula paʻa. ʻOi aku ka laulā o ke ʻano komo no kahi electrode cored a ʻoi aku ka pāpaʻu iki, e hōʻemi ana i ke ʻano o ka puhi ʻana ma nā ala aʻa a i ʻole nā ​​​​hui i kūpono ʻole.

NĀ PALAPALA NOI:

He kūpono ʻo Select EM14KS no kēlā mau noi e pili ana i ka hoʻopili ʻana o nā ipu kaomi a me nā kila kalapona kūkulu e like me A36, A285, A515, a me A516. Pono e hoʻohana ʻia me nā fluxes kūlike ʻole a hiki ke pani ʻia ma nā wahi āpau i hoʻohana ʻia ai kahi uea paʻa, ʻo EM14K electrode.

KEMIKILA HOʻOPUKA MAʻAMAU:

Wt%

C

Mn

P

S

Si

Ti

.06

1.55

.015

.015

.55

.05

NĀ KUMU HOʻOPIʻI I MANAʻO ʻIA:

5/64”

Nā Amps
250

Nā Volts
26-27

WFS (ipm)
90

ESO (i loko)
¾”-1¼”

Ka helu emi ʻana (lb/hr)
6.5

350

29-30

160

11

500

33-34

290

20

3/32”

275

28-29

80

1”-1¼”

8.5

450

32-33

155

15.5

600

37-38

245

24.7

1/8”

400

28-29

68

1”-1¼”

11.5

550

32-33

100

17

750

37-38

150

26.5

5/32”

425

30-31

45

1¼”-1½”

11.5

650

34-35

80

18.5

900

40-42

140

38