Nā Koʻokoʻo Kuʻihao Kalapona ER70S-2, Nā Metala Hoʻopihapiha no ka Uea Kuʻihao Arc Pale Kinoea, Mea Hoʻolako Solder Maikaʻi Loa

Wehewehe Pōkole:

He uea MIG & TiG kiʻekiʻe ʻo ER70S2 no ka hoʻoheheʻe ʻana ma nā ʻano kila palupalu a me ke kalapona āpau, e hana ana i nā hoʻoheheʻe maikaʻi me ka porosity liʻiliʻi.


Nā kikoʻī huahana

Nā Lepili Huahana

He uea MIG & TiG kiʻekiʻe ʻo ER70S2 no ka hoʻoheheʻe ʻana ma nā ʻano kila akahai a me ke kalapona āpau, e hana ana i nā hoʻoheheʻe maikaʻi me ka porosity liʻiliʻi. He uea deoxidized ʻekolu ia (Zirconium, Titanium, a me Aluminum) e lilo ia i koho maikaʻi loa no ka hoʻoheheʻe ʻana ma luna o ka ʻōpala a me ka wili. ʻAʻohe pono o ka flux me kēia huahana.

NĀ PILI MAʻAMAU:

nā paipu a me nā mea ʻeli ma waho o ke kai, nā hana kila kūkulu

Kūlana Kuʻihao: F, V, OH, H I kēia manawa:DCEP
Ikaika Uila, kpsi: 70
Ka ikaika o ka hāʻawi ʻana, kpsi: 58
Elongation ma 2”%: 22

ʻO ke kiʻekiʻe Charpy V-Notch maʻamau: 35 ft.-lb. Ma -20 deg F

Kemika Uea Maʻamau e like me AWS A5.18 (ʻo nā waiwai hoʻokahi ka palena kiʻekiʻe loa)

C Mn Si P S Ni Cr Mo V Cu Ti Zr Al
0.07 0.90-1.40 0.40-0.70 0.025 0.035 0.15 0.15 0.15 0.03 0.50 0.05-0.15 0.02-0.12 0.05-0.15
Nā Kūlana Kuʻihao Maʻamau
Anawaena Kaʻina Hana Volt Nā Amps Kinoea Pale
in (mm)
.035 (0.9) GMAW 28-32 165-200 Hoʻoili Pīpī 98% Argon+2% Oxygen a i ʻole 75% Argon+25% CO2
.045 (1.2) GMAW 30-34 180-220 Hoʻoili Pīpī 98% Argon+2% Oxygen a i ʻole 75% Argon+25% CO2
1/16 (1.6) GMAW 30-34 230-260 Hoʻoili Pīpī 98% Argon+2% Oxygen a i ʻole 75% Argon+25% CO2
.035 (0.9) GMAW 22-25 100-140 Hoʻoili Kaapuni Pōkole 100% CO2 a i ʻole 75% Argon +25% CO2
.045 (1.14) GMAW 23-26 120-150 Hoʻoili Kaapuni Pōkole 100% CO2 a i ʻole 75% Argon +25% CO
1/16 (1.6) GMAW 23-26 160-200 Hoʻoili Kaapuni Pōkole 100% CO2 a i ʻole 75% Argon +25% CO
.035 (0.9) GTAW 13-16 60-100 100% ʻAkekona
.045 (1.14) GTAW 13-16 70-120 100% ʻAkekona
1/16 (1.6) GTAW 12-15 100-125 100% ʻAkekona
3/32 (2.4) GTAW 15-20 125-175 100% ʻAkekona
1/8 (3.2) GTAW 15-20 175-250 100% ʻAkekona

  • Ma mua:
  • Aʻe: