ʻO ke koko kahe Uea Kuʻihao, Papa: A 5.22 E308l T1-1
Nā kikoʻī huahana
| Mea Uea | SS |
| Ka nui no kēlā me kēia ʻōwili | 15 kg |
| Ka hoʻopili ʻana | 15 kg no kēlā me kēia ʻeke |
| Papa | A 5.22 E308L T1-1 |
| ʻAno Pūʻolo | Hoʻopaʻa ʻia ka spool i loko o ka ʻeke polythene a ua wahī ʻia i loko o kahi pahu corrugated |
| Mānoanoa | 1.2MM 1.6MM |
| I kēia manawa | 190-300A |
| Hoʻolōʻihi Uea | 20-25mm (ʻō aku) |
| Nui i loaʻa | 2.00mm,2.4mm |
| Ke ʻano o ka polari | uea DC maikaʻi |
| Kinoea Pale | Kinoea CO2 me ka nui o ke kahe ʻana o 15-20 lita/minuke |
| Nā Waiwai Mekanika Weld | UTS=520N/mm2 Min; Elongation(%)=35% min |
| Kemika metala hoʻoheheʻe | C= 0.035%, Mn=1.65%,P=0.02%,Si=0.50%,S=0.008%,Ni=9.50%,Cr=19.50% |
Wehewehe Huahana
ʻO ke uea kila kila flux cored me ka piʻo paʻa a laumania, me ka detachability slag maikaʻi
Nā noi:
No ka hoʻopili ʻana i nā kila Low Carbon 18-20% Cr/ 8-12% Ni me ka hiki ke hoʻopili maikaʻi loa Ma muli o ke alo o ka ferrite, ʻoi aku ka haʻahaʻa o ka palupalu o ka metala hoʻopili i ka haki ʻana. ʻOi aku ka maikaʻi o nā waiwai mechanical i ke kūlana Welded a ʻoi aku ka maikaʻi o ke kūpaʻa ʻana i ka corrosion intergranular ma muli o ka haʻahaʻa o ka ʻike kalapona.
Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana o nā electrodes welding,nā koʻokoʻo wili, a me nā mea hoʻopau kuʻihao no nā makahiki he 20 a ʻoi.
ʻO kā mākou huahana nui e komo pū me nā electrodes wili kila kila, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili nickel & cobalt alloy, nā uea wili kila māmā & haʻahaʻa alloy, nā uea wili kila kila, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili nickel & cobalt alloy, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.