Uea Kuʻihao Nickel Alloy ERNiCr-3 Mig Welding Wire

Wehewehe Pōkole:

Hoʻohana ʻia ʻo ERNiCr-3 no ka hoʻopili ʻana i nā alloys 600, 601, 690, 800 a me 800HT etc.


Nā kikoʻī huahana

Nā Lepili Huahana

Nikala AlloyUea KuʻihaoʻO ERNiCr-3

Nā Kūlana
EN ISO 18274 – Ni 6082 – NiCr20Mn3Nb
AWS A5.14 – ER NiCr-3

 

Nā Hiʻohiʻona a me nā Noi

Hoʻohana ʻia ka Alloy 82 no ka hoʻopili ʻana i nā alloys 600, 601, 690, 800 a me 800HT etc.

He ikaika kiʻekiʻe ka metala i waiho ʻia a he kūpaʻa maikaʻi hoʻi i ka pala, me ke kūpaʻa ʻana i ka oxidation a me ka ikaika kolo i nā mahana kiʻekiʻe.

He kūpono no nā noi kuʻihao like ʻole ma waena o nā ʻano like ʻolenikalanā mea hao hao, nā kila kila ʻole, nā kila kalapona me ka uhi ʻana.

He kūpono no nā noi mai ka cryogenic a i nā mahana kiʻekiʻe e hana ana i kēia alloy kekahi o nā mea i hoʻohana nui ʻia ma kanikalaʻohana.

ʻO ka ʻōwili papa kikoʻī no nā ʻano hānai uea kiʻekiʻe.

Hoʻohana pinepine ʻia i ka hana mana a me nā ʻoihana petrochemical etc.

Nā Mea Kumu Maʻamau

ʻAla hao 600, ʻAla hao 601, ʻAla hao 690, ʻAla hao 800, ʻAla hao 330*
* He papa inoa hoʻākāka, ʻaʻole piha

 

Ka % o ka hoʻohuihui kemika

C%

Mn%

Fe%

P%

S%

Si%

ka nui loa

2.50

ka nui loa

ka nui loa

ka nui loa

ka nui loa

0.05

3.50

3.00

0.030

0.015

0.50

Cu%

Ni%

Co%

Ti%

Cr%

Nb+Ta%

ka nui loa

67.00

ka nui loa

ka nui loa

18.00

2.00

0.50

minuke

1.00

0.75

22.00

3.00

 

Ikaika Hoʻopaʻa ≥600 MPa
Ikaika Hāʻawi ≥360 MPa
Hoʻolōʻihi ≥30 MPa
Ikaika hopena ≥100 MPa

He kohu wale nā ​​​​waiwai mechanical a hiki ke loli ma muli o ka wela, ke kinoea pale, nā palena kuʻihao a me nā kumu ʻē aʻe.

 

Nā Kinoea Pale

EN ISO 14175 – I1, I3

 

Nā Kūlana Kuʻihao

EN ISO 6947 – PA, PB, PC, PD, PE, PF

 

ʻIkepili Hoʻopili

Anawaena

Kaumaha

ʻŌwili

Ka nui o ka paleta

1.00 mm

1.20 mm

15 Kg

15 Kg

BS300

BS300

72

72

Kuleana: ʻOiai ua hana ʻia nā hana kūpono āpau e hōʻoia i ka pololei o ka ʻike i loko, hiki ke loli kēia ʻike me ka ʻole o ka hoʻolaha ʻana a hiki ke manaʻo ʻia he kūpono no ke alakaʻi maʻamau.

 


  • Ma mua:
  • Aʻe: