Uea hoʻoheheʻe nikala ERNiCrMo-4 Tig wire

Wehewehe Pōkole:

Hoʻohana ʻia ʻo ER-NiCrMo-4 no ka hoʻopili ʻana i nā mea hao me nā ʻano kemika like, ʻo ia hoʻi nā mea like ʻole o nā mea hao nickel-base, nā kila a me nā kila kila ʻole.


Nā kikoʻī huahana

Nā Lepili Huahana

Nikala AlloyUea KuʻihaoUea TigʻO ERNiCrMo-4

 

Nā Kūlana
EN ISO 18274 – Ni 6276 – NiCr15Mo16Fe6W4
AWS A5.14 – ER NiCrMo-4

 

Nā Hiʻohiʻona a me nā Noi

Hoʻohana ʻia ʻo ER-NiCrMo-4 no ka hoʻopili ʻana i nā alloys i loaʻa nā ʻano kemika like, ʻo ia hoʻi nā mea like ʻole onikala-nā mea hoʻohuihui kumu, nā kila a me nā kila kila ʻole.

Ma muli o ke kiʻekiʻe o ka molybdenum, hāʻawi kēia metala i ke kūpaʻa maikaʻi loa i ka nahā ʻana o ke koʻikoʻi a me ka pala, ka pitting a me ka crevice corrosion.

Hoʻohana pinepine ʻia ma nā paipu, nā moku kaomi, nā mea kanu hana kemika, nā kahua aila ma waho, nā hale hana kinoea, ka hana mana a me nā wahi kai, etc.

Nā Mea Kumu Maʻamau

N10276, W.Nr: 2.4819, NiMo16Cr15W, Alloy C4, Alloy C276*
* He papa inoa hoʻākāka, ʻaʻole piha

 

 

Ka % o ka hoʻohuihui kemika
C% Mn% Fe% P% S% Si%  
ka nui loa ka nui loa ka nui loa ka nui loa ka nui loa ka nui loa  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
ka nui loa 93.00 ka nui loa 2.00 ka nui loa    
0.20 minuke 1.00 3.50 1.00    

 

Nā Waiwai Mekanika
Ikaika Hoʻopaʻa ≥690 MPa  
Ikaika Hāʻawi -  
Hoʻolōʻihi -  
Ikaika hopena -  

He kohu wale nā ​​​​waiwai mechanical a hiki ke loli ma muli o ka wela, ke kinoea pale, nā palena kuʻihao a me nā kumu ʻē aʻe.

 

Nā Kinoea Pale

EN ISO 14175 – TIG: I1 (Argon)

 

Nā Kūlana Kuʻihao

EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG

 

ʻIkepili Hoʻopili
Anawaena Ka lōʻihi Kaumaha  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

Kuleana: ʻOiai ua hana ʻia nā hana kūpono āpau e hōʻoia i ka pololei o ka ʻike i loko, hiki ke loli kēia ʻike me ka ʻole o ka hoʻolaha ʻana a hiki ke manaʻo ʻia he kūpono no ke alakaʻi maʻamau.