ʻO AWS E410NiMo -15 Stainless Steel Welding Electrode me ka Low Hydrogen Sodium Coating, Arc Welding Stick

Wehewehe Pōkole:

ʻO G207NiMo (AWS E410NiMo -15) kahi electrode kila kila martensitic me ka uhi sodium hydrogen haʻahaʻa.


Nā kikoʻī huahana

Nā Lepili Huahana

Kuʻihao kila kilaʻElekoda

G207NiMo                                                     

GB/T E410NiMo -15

ʻAWS E410NiMo -15

 

Wehewehe: ʻO G207NiMo kahi electrode kila kila martensitic me ka uhi sodium hydrogen haʻahaʻa. Hoʻohana i ka DCEP (electrode current direct) a hiki ke hoʻopaʻa ʻia ma nā kūlana āpau. Loaʻa i ka papa ʻili nā waiwai anti-cavitation maikaʻi a me nā waiwai anti-one wear. He maʻalahi ke kaʻina hana hoʻopaʻa ʻili, ʻaʻohe pono e hoʻomehana mua ma mua o ka hoʻopaʻa ʻana, ʻaʻohe pono o ka mālama wela ma hope o ka hoʻopaʻa ʻana, a hiki ke mīkini ʻia ka papa ʻili.

Noi: Hoʻohana nui ʻia ia no ka hoʻoponopono ʻana i ka hoʻoheheʻe ʻana o nā mea kila kila 0Cr13Ni4Mo, ka hoʻoponopono ʻana i nā ʻāpana kahe hydropower ma hope o ka hoʻohana ʻana o ka cavitation, a me ka hoʻoheheʻe ʻana i nā ʻāpana kūkulu o ka mea like.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Mn

Si

Cr

Ni

Mo

S

P

≤0.06

≤1.0

≤0.90

11.0 ~ 12.5

4.0 ~ 5.0

0.40 ~ 0.70

≤0.03

≤0.04

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

Mea hoʻāʻo

Ikaika tensile

Mpa

Hoʻolōʻihi

%

Hōʻoiaʻiʻo ʻia

≥760

≥15

 

Manaʻo ʻia kēia manawa:

Anawaena o ke koʻokoʻo

(mm)

3.2

4.0

5.0

Au Kuʻihao

(A)

80 ~ 120

120 ~ 160

150 ~ 190

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 300 ℃ ma mua o ka hana kuʻihao;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka unahi aila, ka wai, a me nā mea haumia ma nā ʻāpana kuʻihao ma mua o ka kuʻihao ʻana.

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana oʻeleka uila hoʻoheheʻes, nā koʻokoʻo wili, a me nā mea hoʻopau wili no nā makahiki he 20 a ʻoi. ʻO kā mākou huahana nui e komo pū me ke kila kilaʻeleka uila hoʻoheheʻes, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili hao nickel & cobalt, nā uea wili kila akahai & haʻahaʻa, nā uea wili kila kila ʻole, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili hao nickel & cobalt, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 