Uea Kuʻihao Kopa AWS ERCU Uea Kuʻihao Keleawe

Wehewehe Pōkole:

He metala keleawe deoxidized ʻo ERCu i hoʻomohala ʻia e hāʻawi i nā waihona paʻa a kiʻekiʻe me ka conductivity uila kiʻekiʻe no ka hoʻohana ʻana i ka hui ʻana a me ke uhi ʻana me nā kaʻina hana inert-gas.


Nā kikoʻī huahana

Nā Lepili Huahana

He metala keleawe deoxidized ʻo ERCu i hoʻomohala ʻia e hāʻawi i nā waihona paʻa a kiʻekiʻe me ka conductivity uila kiʻekiʻe no ka hoʻohana ʻana i ka hui ʻana a me ke uhi ʻana me nā kaʻina hana inert-gas.
Hoʻohana nui ʻia ka uea wili ERCu a me ke koʻokoʻo metala hoʻopihapiha e hana i ke keleawe deoxidized a hoʻoponopono i nā mea hoʻoheheʻe keleawe me nā kaʻina hana gas metal-arc a me ke kinoea tungsten-arc. Hiki ke hoʻohana ʻia hoʻi e hoʻoheheʻe i ke kila galvanized a me ke keleawe deoxidized i ke kila palupalu kahi i ʻole e pono ai nā hui ikaika kiʻekiʻe.
Hoʻohana ʻia ka uea wili ERCu a me ke koʻokoʻo metala hoʻopihapiha e uhi i nā ʻili e pale aku i ka pala. Hoʻohana pinepine ʻia ʻo ERCu no nā ʻōmole billet, nā ʻōwili alakaʻi, nā mea hoʻomehana, nā kiʻi keleawe, nā mea paʻa electrode wili kila, nā kaola kaʻa, a me nā mea hoʻohui keleawe.

Hana kino a me nā waiwai mechanical:
Paʻa-pae 1020 DEG C ka nui 8.9kg/dm ka wikiwiki hoʻonui o 30-40%
ʻO ka ikaika tensile liquidus 1050 DEG C 210-220N/mm2, paʻakikī Brinell 60HB

ʻO ka ERCU Copper Alloy Welding Wire Chemical Composite

Hui Kemika (%)
Nā Kūlana ISO 24373 GB/T9460 BS EN14640 AWS A5.7 DIN1733
Papa HELU. Cu1898 SCu1898 Cu1898 C18980 2.1006
ʻAʻohe Alloy. ʻO CuSn1 ʻO CuSn1 ʻO CuSn1 ERCu SG-CuSn
Cu Minimum 98 Min98 Bal. Minimum 98 Bal.
Al 0.01 Max 0.01 0.01 0.01 Max 0.01
Fe – – 0.05 0.50 Max 0.05
Mn 0.50 ʻOi loa 0.5 0.1~0.5 0.50 0.1~0.5
Ni – – 0.3 – Max 0.3
P 0.15 Max 0.15 0.02 0.15 Max 0.02
Pb 0.02 Max 0.02 0.02 0.02 Max 0.01
Si 0.5 ʻOi loa 0.5 0.5 0.5 0.1~0.5
Sn 1.0 1.0 kiʻekiʻe loa 0.5~1.0 1.0 0.5~1.0
As – – 0.05 – Max 0.05
Huina ʻē aʻe 0.5 ʻOi loa 0.5 0.1 0.5 Max 0.1

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana i nā electrodes wili, nā koʻokoʻo wili, a me nā mea hoʻopau wili no nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me nā electrodes wili kila kila, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili nickel & cobalt alloy, nā uea wili kila māmā & haʻahaʻa alloy, nā uea wili kila kila, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili nickel & cobalt alloy, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 

 

 

 