ʻElektrode Kuʻi Keleawe a me ke Keleawe
T207
GB/T ECuSi-B
AWS A5.6 ECuSi
Wehewehe: He electrode keleawe me ka silicon bronze core a me ka uhi sodium hydrogen haʻahaʻa. E hoʻohana i ka DCEP (direct current electrode positive) me nā waiwai mechanical maikaʻi loa. Loaʻa iā ia ke kūpaʻa maikaʻi i ka pala i nā waikawa inorganic ʻē aʻe ma mua o ka waikawa nitric, ka hapa nui o nā waikawa organik a me ka wai kai.
Hoʻohana: He kūpono ia no ka hoʻopili ʻana i ke keleawe, ke keleawe silicon a me ke keleawe, ka hoʻopili ʻana i nā ʻili o nā paipu mīkini kemika, a pēlā aku.
Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):
| Cu | Si | Mn | Pb | ʻAl+Ni+Zn |
| >92.0 | 2.5 ~ 4.0 | ≤3.0 | ≤0.02 | ≤0.50 |
Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:
| 试验项目 Mea hoʻāʻo | 抗拉强度 Ikaika tensile Mpa | 延伸率 Hoʻolōʻihi % |
| 保证值 Hōʻoiaʻiʻo ʻia | ≥270 | ≥20 |
Manaʻo ʻia kēia manawa:
| Anawaena o ke koʻokoʻo (mm) | 3.2 | 4.0 | 5.0 |
| Au Kuʻihao (A) | 90 ~ 130 | 110 ~ 160 | 150 ~ 200 |
Hoʻolaha:
Nā Mālama:
1. Pono e hoʻomoʻa ʻia ka electrode ma kahi o 300°C no 1 a 2 mau hola ma mua o ka hoʻopili ʻana;
2. Pono e wehe ʻia ka makū, ka ʻaila, nā ʻokikene a me nā mea haumia ʻē aʻe ma luna o ka ʻili o ka weldment ma mua o ka welding.
3. I ka wā e kuʻi ai i ke keleawe silicon a i ʻole ka kuʻi ʻana i ka ʻili ma ke kila, ʻaʻohe pono o ka hoʻomehana mua ʻana. ʻO ka mahana hoʻomehana mua no ka kuʻi ʻana i ke keleawe maʻemaʻe ma kahi o 450°C, a ʻo ka mahana hoʻomehana mua no ka kuʻi ʻana i ke keleawe ma kahi o 300°C;
4. Pono e hoʻohana ʻia ka wiliwili pōkole i ka wā o ka wiliwili ʻana. I ka wā o ka wiliwili multi-layer, pono e hoʻokaʻawale ʻia ka slag ma waena o nā papa.
wehe loa ʻia; ma hope o ka hoʻoheheʻe ʻana, e kuʻi i ka wili me ka hāmare poʻo pālahalaha e hoʻomaʻemaʻe i nā ʻano palaoa, hoʻopau i ke kaumaha, a hoʻomaikaʻi i ka ikaika a me ka plasticity o ka wili.