AWS ENi-1 Maʻemaʻe Nickel Welding Electrode Ni102 Nickel Alloy Electrodes Stick Weld Rods no ka Arc Weld

ʻO ka wehewehe pōkole:

ʻO Ni102 (AWS ENi-1) he nickel electrode maʻemaʻe me ka titanium-calcium coating.Hiki ke hoʻohana ʻia no ka wiliwili kūlana āpau me AC a me DC.


Huahana Huahana

Huahana Huahana

Nickel a me Nickel AlloywiliwiliElectrode

Ni102                                                     

GB/T ENi2061

AWS A5.11 ENi-1

ʻO ka wehewehe: ʻO Ni102 kahi electrode nickel maʻemaʻe me ka titanium-calcium coating.Hiki ke hoʻohana ʻia no ka wiliwili kūlana āpau me AC a me DC.ʻO ka metala i waiho ʻia he mau waiwai mechanical maikaʻi, kūpaʻa wela a me ka pale ʻana i ka corrosion.

Hoʻohana: Hoʻohana ʻia no ka wili ʻana i ka nickel maʻemaʻe (UNS N02200 a i ʻole N02201) ka hoʻoheheʻe ʻana a me ka hoʻolei ʻana i nā mea hao, ka hoʻoheheʻe ʻana i ke kila nickel-composite, ka uhi ʻana o ke kila a me ka hoʻopili ʻana i ke kila like ʻole.

 

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Fe

P

S

Si

Al

Ti

Ni

Cu

'ē aʻe

≤0.10

≤0.7

≤0.7

≤0.020

≤0.015

≤1.2

≤1.0

1.0 ~ 4.0

≥92.0

≤0.2

≤0.5

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

Hua ikaika

Mpa

ʻO ka lōʻihi

%

Hōʻoiaʻiʻo

≥410

≥200

≥18

 

Manaʻo ʻia i kēia manawa:

Anawaena lāʻau

(mm)

2.5

3.2

4.0

Ke au wiliwili

(A)

50 ~ 80

80 ~ 120

130 ~ 170

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 350 ℃ ma mua o ka hana wili;

2. Pono pono e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila, ka wai, a me nā haumia ma nā ʻāpana wili ma mua o ka wili ʻana.

 