Nā Kokola Kuʻi ʻAla Nickel AWS ENiCu-7 Ni70Cu30 Nickel Based Welding Electrodes Manual Metal Arc Electrodes

Wehewehe Pōkole:

ʻO Ni202 (AWS ENiCu-7) kahi electrode alloy Ni70Cu30 Monel me ka uhi ʻana o ka titanium calcium. Hiki ke hoʻohana ʻia no ka AC a me DC.


Nā kikoʻī huahana

Nā Lepili Huahana

ʻElekode Kuʻihao Nickel a me Nickel Alloy

Ni202                                                     

GB/T ENi4060

ʻAWS A5.11 ENiCu-7

Wehewehe: ʻO Ni202 kahi electrode alloy Ni70Cu30 Monel me ka uhi titanium calcium. Hiki ke hoʻohana ʻia no AC a me DC. Loaʻa i ka metala i waiho ʻia ke kūpaʻa maikaʻi i ka haki ma muli o ka ʻike kūpono o ka manganese a me ka niobium. Loaʻa iā ia ka hana kuʻi maikaʻi loa me ka puhi ʻana o ke arc paʻa, ka liʻiliʻi o ka spatter, ka wehe maʻalahi ʻana i ka slag, a me ka weld nani.

Noi: Hoʻohana ʻia no ka hoʻopili ʻana i ka nickel-copper alloy a me ke kila like ʻole, a hiki ke hoʻohana ʻia ma ke ʻano he mea uhi hoʻololi.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Mn

Fe

Si

Nb

Al

Ti

Cu

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤2.5

≤1.0

≤1.0

27.0 ~ 34.0

≥62.0

≤0.015

≤0.020

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

Mea hoʻāʻo

Ikaika tensile

Mpa

Ikaika hāʻawi

Mpa

Hoʻolōʻihi

%

Hōʻoiaʻiʻo ʻia

≥480

≥200

≥27

 

Manaʻo ʻia kēia manawa:

Anawaena o ke koʻokoʻo

(mm)

2.5

3.2

4.0

Au wili

(A)

50 ~ 80

90 ~ 110

110 ~ 150

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 250 ℃ ma mua o ka hana kuʻihao;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila, ka wai, a me nā mea haumia ma nā ʻāpana kuʻihao ma mua o ka kuʻihao ʻana.

 