AWS/ASME A 5.3 E 3003 Aluminum Welding Electrodes

ʻO ka wehewehe pōkole:

No ka wiliwili ʻana i nā alumini i hoʻohui ʻia me ka manganese a me ka magnesium.Maikaʻi nō hoʻi no ka hoʻohui ʻana i nā pae like ʻole o ka alumini a no nā noi wai kai


Huahana Huahana

Huahana Huahana

ʻO kahi papa ʻaoʻao haʻahaʻa me nā huki huki ʻehā, i hoʻolālā ʻia i ke keʻokeʻo me kahi kiʻi gula nani a me nā leo, a me ke aniani akaka e uhi ana i ka ʻili o luna.ʻO kahi hoʻohui nani i hana ʻia i kēlā me kēia wahi noho.He kūpono no ka poʻe e mahalo ana i nā lako nani a nani.

He kūpono ka Gillmore Alberto Collection no nā mea hana i nā hale nani a me nā hale hōʻikeʻike.

Me nā laina maʻemaʻe o kēia manawa a me nā kikoʻī kikoʻī, maʻalahi, kēlā me kēia ʻāpana (he manawa) kahi mea kiʻekiʻe no nā loko lush, i hoʻolālā ʻia me ka noʻonoʻo pono.Loaʻa nā huahana lacquered a pau i ka satin matt white or matt grey, me ka nani metala accenting i ke keleawe a i ʻole chrome ʻeleʻele e hoʻokomo i kahi hiʻohiʻona hou me ka hoʻopiʻi honua.

ʻO kekahi o nā hiʻohiʻona kūʻokoʻa o kēia hōʻiliʻili ʻo ia ke aniani kala like ʻole no kā mākou mau keʻena Alberto āpau no kahi paʻa paʻa o ka maikaʻi ʻole.Eia kekahi, loaʻa nā koho waiho ʻoluʻolu, no ka mea, modular nā ʻāpana a hāʻawi ʻia i nā ʻāpana nui kūpono e hoʻomaha ai i ke kaumaha e hele mai me ka lawe ʻana a me ka hoʻonohonoho ʻana.


DIN: 1732: EL Si-Al Mn

NĀ HIʻona a me nā noi:

No ka wiliwili ʻana i nā alumini i hoʻohui ʻia me ka manganese a me ka magnesium.Maikaʻi nō hoʻi no ka hoʻohui ʻana i nā pae like ʻole o ka alumini a no nā noi wai kai.

Aluminum arc welding electrode me ka mea hookiekie iho.Loaʻa nā helu alumini ʻē aʻe e like me 12% Si, 5% Si a me E 1100, etc.

Unique self lifting slag.

ʻOi aku ka lōʻihi o ke ola keʻokeʻo maʻemaʻe i hoʻokuʻu ʻia i ka flux coating ma mua o nā huahana maʻamau i ke kūpaʻa wai.

Hiki ke hana ʻia ma nā ʻano kala maʻamau.

Loaʻa i loko o nā ʻeke pahu pahu PURE ALUMINIUM i hoʻopaʻa ʻia me ka hermetically a i ʻole nā ​​ʻeke pepa i hoʻopaʻa ʻia no ka lōʻihi o ke ola.

ANALYSIS METAL WELD A PAU (PUNA MAU %):

Ka waihoʻoluʻu Flux: Keʻokeʻo a i ʻole nā ​​kala maʻamau

Si Cu Fe Zn Mn Be Zr Ti Al
0.14 .07 0.23 .002 1.3 .0001 .0004 .009 ʻO Bal.

NA WAIWAI MECHANICAL TYPICAL:

Undiluted Weld metala kiʻekiʻe waiwai a hiki i

Ikaika U'i 34,000 psi (250 N/MPa)

ʻO ka ikaika 20,000 psi (150 N/MPa)

Elongation 10%

WEELDING CURRENT & INSTRUCTION:

Manaʻo ʻia i kēia manawa: DC Reverse (+)
Anawaena (mm) 3/32 (2.5) 1/8 (3.25)
Amperage liʻiliʻi 50 70
Amperage kiʻekiʻe 80 120

Nā ʻenehana welding: E ​​hoʻomaka me ka hoʻohana ʻana i ka ʻāpana o luna o ka pae amperage.E hānai koke i ka electrode a neʻe wikiwiki me ka mālama ʻana i kahi ākea arc kokoke loa.

Nā Kūlana Welding: Flat, Horizontal

NA UKU HOOPAU:

Anawaena(mm) Loihi(mm) Weldmetal/Electrode Electrodesper lb (kg) oWeldmetal Ka manawa o ka waiho ʻana i ka min/lb (kg) AmperageSettings Ka helu hoʻihoʻi
3/32 (2.5) 14″(350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

ELECTRODE PACKAGING & DIMENSIONS:

Anawaena (mm) 3/32 (2.5) 1/8 (3.25) 5/32 (4.0)
Ka lōʻihi (mm) 14″ (350) 14″ (350) 14″ (350)
Electrodes / lb 49 33 23
Electrodes / kg 108 73 51