ʻO ka Brand Tyue Kūlana Kiʻekiʻe Loa ʻo AWS A5.11 ENiCu-7 Nickel Based Welding Electrodes, Nickel Alloy Welding Rods no ka Arc Welding

Wehewehe Pōkole:


Nā kikoʻī huahana

Nā Lepili Huahana

ʻElekode Kuʻihao Nickel a me Nickel Alloy

Ni207                                                     

GB/T ENi4060

ʻAWS A5.11 ENiCu-7

Wehewehe: ʻO Ni207 kahi electrode alloy Monel me ka uhi sodium hydrogen haʻahaʻa. Hoʻohana i ka DCEP (electrode current direct) a loaʻa iā ia ka hana hoʻoheheʻe maikaʻi a me ke kūpaʻa i ka haki.

Hoʻohana: No ka hoʻoheheʻe ʻana i nā kila Monel a i ʻole nā ​​​​​​kila like ʻole. Hiki ke hoʻohana ʻia no ka hoʻopili ʻana i ka papa hoʻololi.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Mn

Fe

Si

Al

Ti

Cu

Nb

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤1.0

≤1.0

27.0 ~ 34.0

≤2.5

≥62.0

≤0.015

≤0.020

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

Mea hoʻāʻo

Ikaika tensile

Mpa

Ikaika hāʻawi

Mpa

Hoʻolōʻihi

%

Hōʻoiaʻiʻo ʻia

≥480

≥200

≥27

 

Manaʻo ʻia kēia manawa:

Anawaena o ke koʻokoʻo

(mm)

3.2

4.0

Au wili

(A)

90 ~ 110

110 ~ 150

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 2 hola ma kahi o 300 ℃ ma mua o ka hana kuʻihao;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila, ka wai, a me nā mea haumia ma nā ʻāpana kuʻi ma mua o ka kuʻi ʻana. E hoʻāʻo e hoʻohana i kahi ʻāʻī pōkole e kuʻi ai.

 