ʻO AWS ER308L Uea Kuʻihao Kila ʻOle MIG a me TIG Nā Koʻokoʻo Kuʻihao

Wehewehe Pōkole:

He kiʻekiʻe ka pono o ka uea wili kila kila, a he maikaʻi ka hana loea wili ʻana i nā ʻoihana āpau. Hoʻohana nui ʻia lākou i nā ʻoihana: nā hale kūkulu, nā kaʻa, nā ʻenekinia alahaka, nā mīkini mining, nā alahao, nā paipu ʻaila, nā lako hana kaomi kinoea, nā lako mana, a pēlā aku.


Nā kikoʻī huahana

Nā Lepili Huahana

Ka Hoʻokaʻawale ʻana o AWS: AWS 5.9

WEHEWEHE:

He kiʻekiʻe ka pono o ka uea wili kila kila, a he maikaʻi ka hana loea wili ʻana i nā ʻoihana āpau. Hoʻohana nui ʻia lākou i nā ʻoihana: hale kūkulu, kaʻa, ke ʻenekinia alahaka, nā mīkini mining, ke alahao, ka paipu ʻaila, nā lako hana kaomi kinoea, nā lako mana, a pēlā aku.

HELU HOʻOHĀLIKE & NUI:

1. Hoʻolako hale hana lawelawe OEM.

2. Kumu hoʻohālike: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi a pēlā aku.

3. Ka nui o ke uea MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4. Ka nui o ka uea TIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.

HOʻOLAUNA:

Hāʻawi mākou i nā ʻano uea kuʻihao kila kila like ʻole, me ka uea kuʻihao paʻa Mig, ka uea kuʻihao Tig rod a me ka uea kuʻihao submerged-arc, nā mea āpau o ke ʻano kiʻekiʻe a kūʻai ʻia aku ma ka honua holoʻokoʻa.

Koe wale nō ka 308 a me ka 309, hāʻawi pū mākou i ka 304, 321, 347, 316L, 310, 2209, a me 201. A me nā kikoʻī kūikawā e like me 318L, 904L, 2594, NiCrMo-3, Ni1.

KA HOʻOPILI ʻANA:

ʻO ka hoʻopili ʻana i ka uea kuʻihao Mig (ʻeke spool a me ka pahu)

Anawaena: 0.8 - 2.0mm

Pūʻolo: 1 kg/wili, 5 kg/wili, 15 kg/wili, 20 kg/wili, 100 kg/pahu, 200 kg/pahu

ʻO ka hoʻopili ʻana i ka uea hoʻoheheʻe lāʻau Tig (paipu plastik)

Anawaena: 1.0 - 5.0mm

Pūʻolo: 5 kg/ʻeke

Uea kuʻihao arc i hoʻokomo ʻia i loko o ka wai

Anawaena: 2.5 - 5.0mm

Pūʻolo: 20kg/ʻeke, 25 kg/ʻeke

Hoʻokipa ʻia ka ʻōpala kūlike a me ka OEM!

NĀ HUI KEMIKALA O KA WEHE WEHE KILA KINO:

Kumu Hoʻohālike Helu.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

NĀ ʻANO MĀKĀNIA O KA WEHE WEHE:

Kumu Hoʻohālike Helu.

Ikaika tensile Rm(Mpa)

Ka ikaika o ka hua Rel a i ʻole Rp0.2 (Mpa)

Hoʻolōʻihi

(%)

Kumu Hoʻohālike Helu.

Ikaika tensile Rm(Mpa)

Ka ikaika o ka hua Rel a i ʻole Rp0.2 (Mpa)

Hoʻolōʻihi

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

ʻO ka haku mele ʻana o ka uea kuʻi kila kila TIG a me MIG

YB5092-2005

AWS

Ka % o ka hoʻohuihui kemika

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Cu 1.80

H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Cu;3 Nb;0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana i nā electrodes wili, nā koʻokoʻo wili, a me nā mea hoʻopau wili no nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me nā electrodes wili kila kila, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili nickel & cobalt alloy, nā uea wili kila māmā & haʻahaʻa alloy, nā uea wili kila kila, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili nickel & cobalt alloy, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana i nā electrodes wili, nā koʻokoʻo wili, a me nā mea hoʻopau wili no nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me nā electrodes wili kila kila, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili nickel & cobalt alloy, nā uea wili kila māmā & haʻahaʻa alloy, nā uea wili kila kila, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili nickel & cobalt alloy, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.


  • Ma mua:
  • Aʻe: