E70C-6M Carbon Steel Flux Cored Arc Welding Electrodes Flux Core Welding Wire

ʻO ka wehewehe pōkole:

ʻO E70C-6M uea hoʻoheheʻe metala i hui pū ʻia i ka maikaʻi o nā uea paʻa (GMAW) me nā kiʻekiʻe o ka huahana kiʻekiʻe o nā uea flux-cored (FCAW) - haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa, kiʻekiʻe efficiencies, ʻaʻohe slag e hoʻomaʻemaʻe a wehe ʻia-me nā mea maikaʻi a pau. ʻO nā uea ma luna o nā uea paʻa-ʻaʻohe "'ūhā anu" a i ʻole ka hui ʻana o ka ʻaoʻao ʻaoʻao, ʻoi aku ka maikaʻi o ka pulupulu maʻemaʻe me 75-80% argon/balance carbon dioxide, ʻoi aku ka wikiwiki o ka huakaʻi hele no ka nui o ka waihona.


Huahana Huahana

Huahana Huahana

ʻO E70C-6M uea hoʻoheheʻe metala i hui pū ʻia i ka maikaʻi o nā uea paʻa (GMAW) me nā kiʻekiʻe o ka huahana kiʻekiʻe o nā uea flux-cored (FCAW) - haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa, kiʻekiʻe efficiencies, ʻaʻohe slag e hoʻomaʻemaʻe a wehe ʻia-me nā mea maikaʻi a pau. ʻO nā uea ma luna o nā uea paʻa-ʻaʻohe "'ūhā anu" a i ʻole ka hui ʻana o ka ʻaoʻao ʻaoʻao, ʻoi aku ka maikaʻi o ka pulupulu maʻemaʻe me 75-80% argon/balance carbon dioxide, ʻoi aku ka wikiwiki o ka huakaʻi hele no ka nui o ka waihona.Ua kūpono ʻo E70C-6M i nā noi kahi e pono ai ke kiʻekiʻe o ka manganese a me ke kiʻekiʻe kiʻekiʻe, e like me ke alo o ka unahi wili kaumaha a i ʻole nā ​​mea haumia ʻoluʻolu, a i ʻole ke makemake ʻia ka hoʻomaʻemaʻe ʻana o ka weld bead.ʻOi aku ka maikaʻi o kēia huahana ma ka wiliwili kumu nui, akā ʻoi aku ka maikaʻi ma nā kūlana koi kiʻekiʻe e like me ka hana ʻana i ka metala ʻoi aku ke kaumaha, ka hana hoʻolālā, wili paipu a me ka wili ʻana o nā mea hoʻomehana wai wela.

Papa AWS: E70C-6M Hōʻoia: AWS A5.18/A5.18M:2005
Huina: E70C-6M ASME SFA A5.18

 

Kūlana Welding: F, H, V, OH .035-1/16”
F, H 5/64”-1/8”
I kēia manawa:
DCEP

 

Ka ikaika uʻi, kpsi: 70 100% CO2
Ka ikaika o ka hua, kpsi: 58 100% CO2
Elongation ma 2”%: 22 100% CO2

ʻO ke Kemika Wire maʻamau e like me AWS A5.18 (ʻoi aku ka nui o nā waiwai hoʻokahi)

C Mn Si S P Ni Cr Mo V Cu  
0.12 1.75 0.90 0.03 0.03 0.50 0.20 0.30 0.08 0.50  
Nā Kūlana Kūlohelohe maʻamau
Anawaena Kaʻina hana Volt Amps Ke kinoea pale
in (mm)
.035 (0.9) GMAW 24-35 160-250 75-95% Ar / kaulike Co2, 35-50cfh
.045 (1.2) GMAW 37-33 180-330 75-95% Ar / kaulike Co2, 35-50cfh
.052 (1.3) GMAW 25-35 220-460 75-95% Ar / kaulike Co2, 35-50cfh
1/16 (1.6) GMAW 26-37 240-520 75-95% Ar / kaulike Co2, 35-50cfh
5/64 (2 ) GMAW 27-36 240-550 75-95% Ar / kaulike Co2, 35-50cfh
3/32 (2.4 ) GMAW 28-36 350-550 75-95% Ar / kaulike Co2, 35-50cfh
7/64 (2.78 ) GMAW 27-34 400-600 75-95% Ar / kaulike Co2, 35-50cfh
1/8 (3.2) GMAW 26-32 95-145 75-95% Ar / kaulike Co2, 35-50cfh

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. ma 2000. Ua hana mākou i ka hana ʻana i nā electrodes welding,lāʻau wiliwili, a me ka welding consumables no ka oi ma mua o 20 makahiki.

ʻO kā mākou huahana nui e pili ana i nā electrodes kuʻekuʻe, carbon steel welding electrodes. alumini wili uwea, submerged arc welding.uea, nickel & cobalt alloy uea, keleawe wiliwili uea, TIG & MIG wiliwili uea, tungsten electrodes, carbon gouging electrodes, a me na mea wiliwili 'ē aʻe a me nā mea hoʻohana.