Nā Koʻokoʻo Kuʻihao Kela Kalapona ER70S-3, Nā Metala Hoʻopihapiha no ka Uea Kuʻihao Arc Pale Kinoea, Uea Tig a me Mig

Wehewehe Pōkole:

He uea MIG hana maʻamau ka ER70S3 i kūpono no nā hana hoʻopili kila kalapona he nui.


Nā kikoʻī huahana

Nā Lepili Huahana

Nā metala hoʻopihapiha kila kalapona ER70S-3 no ka hoʻoheheʻe ʻana i ke kinoea pale ʻia

He uea MIG hana maʻamau ʻo ER70S3 i kūpono no nā noi wili hao kalapona he nui. He uea deoxidized silicon a me manganese ia e hana maikaʻi loa ai no ka hana ʻana maʻamau. Pono kēia huahana i kahi kinoea pale.

Nā Hoʻohana Maʻamau: hana maʻamau, lako metala, pepa metala, hana hao hoʻonaninani, lako mahiʻai

Papa AWS: ER70S3 Palapala hōʻoia: AWS A5.18/A5.18M:2005
Mea hao: ER70S3 ASME SFA A5.18

 

Kūlana Kuʻihao: F, V, OH, H I kēia manawa:
MIG-DCEP
TIG-DCEN

 

Ikaika Uila, kpsi: 70
Ka ikaika o ka hāʻawi ʻana, kpsi: 58
Elongation ma 2”%: 22

Kemika Uea Maʻamau e like me AWS A5.18 (ʻo nā waiwai hoʻokahi ka palena kiʻekiʻe loa)

C Mn Si P S Ni Cr Mo V Cu
0.06-0.15 0.90-1.40 0.45-0.75 0.025 0.035 0.15 0.15 0.15 0.03 0.50
Nā Kūlana Kuʻihao Maʻamau
Anawaena Kaʻina Hana Volt Nā Amps Kinoea Pale
in (mm)
.035 (0.9) GMAW 28-32 165-200 Hoʻoili Pīpī 98% Argon+2% Oxygen a i ʻole 75% Argon+25% CO2
.045 (1.2) GMAW 30-34 180-220 Hoʻoili Pīpī 98% Argon+2% Oxygen a i ʻole 75% Argon+25% CO2
1/16 (1.6) GMAW 30-34 230-260 Hoʻoili Pīpī 98% Argon+2% Oxygen a i ʻole 75% Argon+25% CO2
.035 (0.9) GMAW 22-25 100-140 Hoʻoili Kaapuni Pōkole 100% CO2 a i ʻole 75% Argon +25% CO2
.045 (1.2) GMAW 23-26 120-150 Hoʻoili Kaapuni Pōkole 100% CO2 a i ʻole 75% Argon +25% CO
1/16 (1.6) GMAW 23-26 160-200 Hoʻoili Kaapuni Pōkole 100% CO2 a i ʻole 75% Argon +25% CO
1/16 (1.6) GTAW 12-15 100-125 100% ʻAkekona
3/32 (2.4) GTAW 15-20 125-175 100% ʻAkekona
1/8 (3.2) GTAW 15-20 175-250 100% ʻAkekona

 


  • Ma mua:
  • Aʻe: