Uea Hoʻopili Mea Hoʻopihapiha RBCuZn-B (Nickel Bronze)

Wehewehe Pōkole:

Ua like ka metala hoʻopihapiha brazing RBCuZn-B Nickel Bronze (RBCuZn-B) me ke keleawe naval akā loaʻa ka manganese a me ka hao e hoʻonui ai i ka paʻakikī a me ka ikaika o ka waihona weld.


Nā kikoʻī huahana

Nā Lepili Huahana

Ua like ka metala hoʻopihapiha brazing RBCuZn-B Nickel Bronze (RBCuZn-B) me ke keleawe naval akā aia ka manganese a me ka hao e hoʻonui ai i ka paʻakikī a me ka ikaika o ka waihona weld. Loaʻa pū kekahi iā ia ka nickel e hōʻoiaʻiʻo ana i ka hoʻolaha like ʻana o ka hao i loko o ka waihona. Pono e hoʻohana ʻia kahi lapalapa kūlike ʻole a i ʻole ka lapalapa oxidizing iki a me kahi flux boric acid/boric type.

Papa AWS: RBCuZn-B Palapala hōʻoia: AWS A5.8/A5.8M:2011
Mea hoʻohuihui: RBCuZn-B ASME SFA A5.8

 

Kūlana Hoʻopaʻa: H, V Ka Pae Hoʻoikaika:
1620-1800⁰F

 

Ikaika Uila, kpsi: 60-78
% Hoʻolōʻihi, min: 25

 

Kiko Heheʻe 1620⁰F Hoʻopaʻa ʻana 1590⁰F Paʻakikī Brinell 80-110

Kemika Uea maʻamau e like me AWS A5.8 (ʻo nā waiwai hoʻokahi ka palena kiʻekiʻe loa)

Cu Zn Sn Fe Mn Ni Pb Al Si ʻĒ aʻe
56.0-60.0 Rem 0.80-1.10 0.25-1.20 0.01-0.50 0.20-0.80 0.05 0.01 0.04-0.20 0.50

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana i nā electrodes wili, nā koʻokoʻo wili, a me nā mea hoʻopau wili no nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me nā electrodes wili kila kila, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili nickel & cobalt alloy, nā uea wili kila māmā & haʻahaʻa alloy, nā uea wili kila kila, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili nickel & cobalt alloy, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 

 

 

 