Uea Kuʻi Paʻa ER410NiMo

Wehewehe Pōkole:

He uea paʻa kila kila martensitic ʻo ER410NiMo me ka hoʻohui kemika e hōʻike ana i 11.0 - 12.5% ​​Cr, 4.0 - 5.0% Ni, a me 0.40 - 0.70% Mo.

Nā kikoʻī huahana

Nā Lepili Huahana

Kūlana pane

-NB/T 47018.3-2017 S410NiMo
-GB/T 29713-2013 S410NiMo
-AWS A5.9M-2022 ER410NiMo
-ASME SFA-5.9M-2023 ER410NiMo
-YB/T 5092-2016 H05Cr12Ni4Mo
Mea like: 1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM

Wehewehena

He uea paʻa kila kila martensitic ʻo ER410NiMo me ka hoʻohui kemika e hōʻike ana i 11.0 - 12.5% ​​Cr, 4.0 - 5.0% Ni, a me 0.40 - 0.70% Mo. He kūpono ia no ka hoʻoheheʻe ʻana i pale ʻia e ke kinoea (e like me TIG/MIG) ma nā kūlana āpau. I ka wā o ka hoʻoheheʻe ʻana, paʻa ka ʻāʻī, a hōʻike ka metala i waiho ʻia i ke kūpaʻa cavitation maikaʻi loa, ke kūpaʻa one.
a me nā waiwai mechanical. ʻAʻole pono ka hoʻomehana mua ʻana ma mua o ka hoʻoheheʻe ʻana; ua ʻōlelo ʻia ka mālama wela ma hope o ka hoʻoheheʻe ʻana (PWHT) ma 580 ~ 620 ℃ no 2 mau hola (a ukali ʻia e ka hoʻoluʻu ea, AC) e like me nā koi o ka noi. Hiki ke mīkini ʻia ka metala i waiho ʻia a kūpono no nā lako hana kaomi.

Noi

Hoʻolālā ʻia no ka hoʻoheheʻe ʻana i ke kila hoʻolei ASTM CA6NM, ke kila kila 410/410S/405, a me nā kila moʻo 13%Cr - 4%Ni like. ʻO nā noi maʻamau e komo pū me nā lako kaomi (e kūlike ana i nā kūlana ipu kaomi), nā lau turbine, nā valves, nā paipu kaomi kiʻekiʻe, a me nā ʻāpana kūkulu e pono ai ka pale ʻana i ka pala a me ka ʻaʻahu.

Ka Hoʻohui Kemika o ka Metala Welded (%)

ʻElemene C Cr Ni Mo Mn Si P S Cu
Koi ≤0.06 11.0-12.5 4.0-5.0 0.40-0.70 ≤1.00 ≤0.60 ≤0.050 ≤0.020 ≤0.75
Hopena Hoʻāʻo 0.011 12.21 4.70 0.54 0.58 0.47 0.016 0.008 0.01

 

Nā Waiwai Mekanika o ka Metal i Waiho ʻia

Inoa Hoʻāʻo Ikaika Tensile (MPa) Hoʻolōʻihi% X-Ray Hoʻāʻo hopena (+20 ℃)J Paʻakikī HB
Koi ≥760 ≥15 Papa I – –
Hopena Hoʻāʻo 830 18 Papa I 65 250-310

Ka Palena Kuʻi i Manaʻo ʻia

Kinoea Pale: Argon (Ar) a i ʻole Ar + 1-2% O2 (no ka hoʻoheheʻe TIG / MIG, hoʻoponopono e like me nā kaʻina hana kikoʻī).

 

Hoʻolaha

1. E hōʻoia i ka maʻemaʻe o ka ʻili o ka uea a ʻaʻohe aila, popo, a i ʻole ka makū ma mua o ka hoʻohana ʻana e pale aku i ka hoʻopilikia ʻana i ka maikaʻi o ka hoʻoheheʻe ʻana.

2. E mālama i ka maʻemaʻe o ke kinoea a me ka nui o ke kahe kūpono e pale aku ai i ka porosity a me ka haki ʻana i hoʻokomo ʻia e ka hydrogen.