ʻO Tyue Brand Best Arc Welding Electrodes AWS ENiCrFe-1 Nickel Welding Rod, Welding Stick

Wehewehe Pōkole:

He electrode nickel-based ʻo Ni307-1 (AWS ENiCrFe-1) me ka uhi haʻahaʻa hydrogen sodium. E hoʻohana i ka DCEP (direct current electrode positive).


Nā kikoʻī huahana

Nā Lepili Huahana

ʻElekode Kuʻihao Nickel a me Nickel Alloy

Ni307-1                                                     

GB/T ENi6062

AWS A5.11 ENiCrFe-1

Wehewehe: He electrode nickel ka Ni307-1 me ka uhi sodium hydrogen haʻahaʻa. E hoʻohana i ka DCEP (direct current electrode positive). ʻOiai aia ka Nb i loko o ka weld, he plasticity maikaʻi ko ka metala i waiho ʻia a me ke kūpaʻa i ka haki.

Hoʻohana: Hoʻohana ʻia no ka hoʻoheheʻe ʻana i nā mea hao nickel-chromium-hao (e like me UNS N06600, UNS N06601) a me ka hoʻopili ʻana i ke kila. Loaʻa iā ia nā waiwai hoʻoheheʻe metala like ʻole. Hiki ke hoʻohana ʻia ma kahi mahana hana o 980°C, akā i ka wā e ʻoi aku ai ka mahana ma mua o 820°C, e emi ana ke kūpaʻa a me ka ikaika o ka oxidation.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Mn

Fe

Si

Cu

Ni

Cr

Nb + Ta

S

P

ʻĒ aʻe

≤0.08

≤3.5

≤11.0

≤0.8

≤0.5

≥62.0

13.0 ~ 17.0

0.5 ~ 4.0

≤0.015

≤0.020

≤0.50

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

Mea hoʻāʻo

Ikaika tensile

Mpa

Ikaika hāʻawi

Mpa

Hoʻolōʻihi

%

Hōʻoiaʻiʻo ʻia

≥550

≥360

≥27

 

 

Manaʻo ʻia kēia manawa:

Anawaena o ke koʻokoʻo

(mm)

2.5

3.2

4.0

5.0

Au wili

(A)

60 ~ 90

80 ~ 110

110 ~ 150

130 ~ 180

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 300 ℃ ma mua o ka hana kuʻihao;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila, ka wai, a me nā mea haumia ma nā ʻāpana kuʻi ma mua o ka kuʻi ʻana. E hoʻāʻo e hoʻohana i kahi ʻāʻī pōkole e kuʻi ai.

 

 