ʻElekoda kila kila AF2209-15 (AWS E2209-15) me ka uhi haʻahaʻa hydrogen. Nā koʻokoʻo no ka hoʻoheheʻe ʻana

Wehewehe Pōkole:

ʻO AF2209-15 (AWS E2209-15) he electrode kila kila duplex haʻahaʻa loa me ka naikokene kalapona me ka uhi hydrogen haʻahaʻa.


Nā kikoʻī huahana

Nā Lepili Huahana

Kuʻihao kila kilaʻElekoda

AF2209-15

GB/T E2209-15

ʻAWS A5.4 E2209-15

Wehewehe: ʻO AF2209-15 kahi electrode kila kila duplex haʻahaʻa loa me ka naikokene kalapona me ka uhi hydrogen haʻahaʻa. E hoʻohana i ka DCEP (electrode current direct). Maikaʻi loa ka hana hana. No ka mea, loaʻa iā ia ka molybdenum a me ka naikokene, a haʻahaʻa loa ka nui o ke kalapona, loaʻa i ka metala i waiho ʻia ke kūpaʻa maikaʻi i ka haki a me ke kūpaʻa i ka palaho, ʻoi aku ka pale ʻana i ka palaho koʻikoʻi.

Hoʻohana: Hoʻohana nui ʻia no ka hoʻoheheʻe ʻana i ke ʻano like o nā mea kila kila kalapona haʻahaʻa loa i nā ʻoihana petroleum a me hydraulic. E like me ka hoʻoheheʻe ʻana o ke kila kila duplex 022Cr22Ni5Mo3N.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

Mea hoʻāʻo

Ikaika tensile

Mpa

Hoʻolōʻihi

%

Hōʻoiaʻiʻo ʻia

≥690

≥20

 

Manaʻo ʻia kēia manawa:

Anawaena o ke koʻokoʻo

(mm)

2.5

3.2

4.0

5.0

Au Kuʻihao

(A)

50 ~70

80 ~ 110

130 ~ 150

160 ~ 200

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 250 ℃ ma mua o ka hana kuʻihao;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka unahi aila, ka wai, a me nā mea haumia ma nā ʻāpana kuʻihao ma mua o ka kuʻihao ʻana.

 

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana oʻeleka uila hoʻoheheʻes, nā koʻokoʻo wili, a menā mea hoʻopau kuʻihaono nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me nā electrodes wili kila kila, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili nickel & cobalt alloy, nā uea wili kila māmā & haʻahaʻa alloy, nā uea wili kila kila, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili nickel & cobalt alloy, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 

 