ʻO AF2209-16 (AWS E2209-16) kahi mea hoʻoheheʻe kila kila-haʻahaʻa loa i loaʻa i ka duplex stainless steel me ka titanium-calcium coating.


Huahana Huahana

Huahana Huahana

Kuʻihao KuʻihaoElectrode

AF2209-16                               

GB/T E2209-16

AWS A5.4 E2209-16

ʻO ka wehewehe ʻana: ʻO AF2209-16 kahi mea hoʻoheheʻe kiʻekiʻe kiʻekiʻe o ka carbon nitrogen-containing duplex stainless steel electrode me ka titanium-calcium coating.Hiki ke hoʻohana ʻia no ka AC a me DC me ka hana maikaʻi loa.No ka mea he molybdenum a me ka naikokene, a he haʻahaʻa loa ka maʻiʻo kalapona, ʻoi aku ka maikaʻi o ka pale ʻana i ka metala i waiho ʻia a me ka pale ʻana i ka corrosion, ʻoi aku ka ikaika o ke kūpaʻa corrosion.

Noi: Hoʻohana nui ʻia ia no ka wili ʻana i ke ʻano like o ka ultra-low carbon stainless steel material i loko o ka ʻaila a me nā ʻoihana hydraulic.E like me ke kuʻi ʻana o 022Cr22Ni5Mo3N duplex stainless steel.

 

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

ʻO ka lōʻihi

%

Hōʻoiaʻiʻo

≥690

≥20

 

Manaʻo ʻia i kēia manawa:

Anawaena lāʻau

(mm)

2.5

3.2

4.0

5.0

Ke au wiliwili

(A)

50 ~70

80 ~ 110

130 ~ 150

160 ~ 200

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 250 ℃ ma mua o ka hana wili;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila unahi, ka wai, a me nā haumia ma nā ʻāpana wili ma mua o ka wili ʻana.

 

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. ma 2000. Ua hana mākou i ka hana ʻana owiliwili uilas, lāʻau wiliwili, awiliwili mea hoopauno nā makahiki ʻoi aku ma mua o 20.

ʻO kā mākou huahana nui he kila kilawiliwili uilas, kalapona kila kuʻihao electrodes, haʻahaʻa wili kuʻihao electrodes, surfacing kuʻihao electrodes, nickel & cobalt kuʻihao kuʻihao electrodes, mild kila & haʻahaʻa wili kuʻihao uea, kuhiliʻole kila kuʻihao uea, kinoea-pale flux cored uea, aluminika kuʻihao uwea, submerged arc kuʻihao. .uea, nickel & cobalt alloy uea, keleawe wiliwili uea, TIG & MIG wiliwili uea, tungsten electrodes, carbon gouging electrodes, a me na mea wiliwili 'ē aʻe a me nā mea hoʻohana.

 

 