ʻElektrode Hoʻopaʻa Paʻakikī AWS A5.13/AME A5.13 ECoCr-C

Wehewehe Pōkole:

ʻO ka ʻili paʻakikī o nā poʻo valve, nā apo sila o ka pamu kiʻekiʻe a me nā ʻāpana o nā mea wili.


Nā kikoʻī huahana

Nā Lepili Huahana

WEHEWEHE:

ʻO ka electrode i uhi ʻia ʻo COBALTHARD 1FC ka mea hoʻohuihui paʻakikī kiʻekiʻe loa i ka hui o nā mea hoʻohuihui cobalt i hoʻohana ʻia no ka ʻaʻahu abrasive wela kiʻekiʻe e pili ana me ka pala. Loaʻa i nā waihona o kēia mea hoʻohuihui ka nui o nā carbide chromium e hoʻopilikia i ke kūpaʻa ʻaʻahu abrasive maikaʻi loa. ʻO ka hoʻohui ʻana o ka tungsten e hoʻonui i ka paʻakikī wela kiʻekiʻe a me ka paʻakikī matrix no ka hoʻopili maikaʻi loa a me ke kūpaʻa ʻana i ka ʻaʻahu ʻana i nā ʻāpana paʻa. Hoʻopili maikaʻi ia me nā kila āpau, me ke kila kila.

NĀ PALAPALA NOI:

ʻO ka ʻili paʻakikī o nā poʻo valve, nā apo sila o ka pamu kiʻekiʻe a me nā ʻāpana o nā mea wili.

PAʻAKIKĪ O KA MEA HOʻOHANA ʻIA: 50 – 56 HRC (520- 620 Hv)

KA HOʻOHUI KEMIKALA MAʻAMAU O KA MEA WELD (%):

C Si Mn Cr W Co
2.15 0.47 1.03 31.25 12.72 Bal

KŪLANA HOʻOKUʻI: PĀLAHALAHA, KUMU I LUNA, MA LUNA

NĀ NUI I LOAʻA A ME NĀ AU I MANAʻO ʻIA (DC +):

Ka nui (diameter mm) 3.2 4.0 5.0
Ka lōʻihi (mm) 350 350 350
Ka Pae o kēia Manawa (Amp) 90 – 120 110 – 150 140 – 180

NĀ MEA E PILI ANA I KA HOʻOHANA ʻANA:

E hoʻomehana mua ma 300ºC a ʻoi aku paha ma ke ʻano laulā.

E hoʻohana i nā lāʻau hōʻike wela PHILARC a i ʻole ke ana wela PHILARC interpass e hoʻoholo ai inā ua loaʻa ka mahana kūpono ma mua o ka hoʻopili ʻana.

He mea pono ke hoʻomehana ma hope o ka hoʻomehana ʻana ma 600ºC a e hoʻomālielie i ka hoʻomaʻalili ma hope o ka kuʻi ʻana e pale ai i ka nahā.

E hoʻomaloʻo i nā electrodes ma 150-200ºC no 30 - 60 mau minuke ma mua o ka hoʻohana ʻana. E hoʻohana i nā umu hoʻomaloʻo lawe lima PHILARC.