Paʻa Paʻa Welding Electrode DIN 8555 (E10-UM-65-GRZ) Paʻa Paʻa Paʻa ʻAno ʻAno: TY-C LEDURIT 67 Arc Welding Stick

ʻO ka wehewehe pōkole:

ʻO DIN 8555 (E10-UM-65-GRZ) kahi mea hoʻolale kiʻekiʻe kiʻekiʻe kiʻekiʻe SMAW electrode no ka hardsurfacing.


Huahana Huahana

Huahana Huahana

Electrode welding paʻakikī

 

Kūlana: DIN 8555 (E10-UM-65-GRZ)

ʻAno ʻAno: TY-C LEDURIT 67

 

Hōʻike a me ka noi:

· Kākoʻo kumu hoʻihoʻi kiʻekiʻe SMAW electrode no ka hardsurfacing.

· ʻOi aku ka paʻakikī o ka ʻili ʻana o nā ʻāpana i ka abrasion kaumaha a me ka hopena haʻahaʻa.

· He kūpono no nā papa paʻakikī hope loa ma hope o ka papa pale.

· ʻO nā ʻāpana mea kanu Sinter, hoʻohana i nā kaola a me nā papa, nā kaola ʻōpala, ka umu ahi, nā ʻōnaehana hoʻouka, nā umu sima, nā niho bakeke a me nā lehelehe, nā pale.

 

Hoʻohui kemika o ka metala i waiho ʻia(%):

 

C

Si

Mn

Cr

B

DIN

Maʻiʻo C kiʻekiʻe a me ka maʻiʻo Cr

Maʻamau

3.5

1.0

1.8

35

1.0

 

ʻO ka paʻakikī o ka metala i waiho ʻia:

Waihona weld maʻemaʻe

(HRC)

1 papa ma 0.15% kila

(HRC)

2 papa ma 0.15% kila

(HRC)

62 – 65

59 – 63

61 – 64

 

Nā ʻano maʻamau:

· Microstructure Martensitic+Austenite+Carbides

· Mīkini Mīkini wale

· Hoʻomaʻa hou i ka Redry no 2 mau hola ma 300 ℃ ma mua o ka hoʻohana ʻana.