ʻO AWS E10015-G (J707Ni) Laʻau Kuʻi Uila Kila Haʻahaʻa

Wehewehe Pōkole:

He ʻelekole kila ikaika kiʻekiʻe ʻo J707Ni (AWS E10015-G) me ka uhi sodium haʻahaʻa.


Nā kikoʻī huahana

Nā Lepili Huahana

ʻO ke kinikini haʻahaʻaKuʻi kilaʻElekoda

J707Ni                               

GB/T E7015-G

ʻAWS E10015-G

 

Wehewehe: He electrode kila ikaika kiʻekiʻe ʻo J707Ni me ka uhi sodium haʻahaʻa-hydrogen. Hoʻohana i ka DCEP (electrode au pololei maikaʻi) a hiki ke hoʻopaʻa ʻia ma nā kūlana āpau. He maikaʻi nā waiwai mechanical o ka metala i waiho ʻia. Ke hoʻohālikelike ʻia me ka electrode J707, ʻo ka hiʻohiʻona nui o J707Ni ʻo ia ka paʻakikī o ka mahana haʻahaʻa a me ke kūpaʻa ʻana i ka haki.

Noi: Hoʻohana ʻia no ka hoʻopili ʻana i nā ʻano kila ikaika haʻahaʻa o nā pae ikaika like, e like me 14MnMoVB, WEL-TEN70 a me Iapana HW56 a me nā ʻano kila ikaika haʻahaʻa ʻē aʻe.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Si

Mn

Ni

Mo

Cr

S

P

≤0.10

≤0.60

≥1.00

1.80 ~ 2.20

0.40 ~ 0.60

≤0.20

≤0.030

≤0.030

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

 

Mea hoʻāʻo

 

Ikaika tensile

Mpa

 

Ikaika hāʻawi

Mpa

 

Hoʻolōʻihi

%

 

Ka waiwai hopena (J)

-40℃

-50℃

 

Hōʻoiaʻiʻo ʻia

≥690

≥590

≥15

—

≥27

 

Ua hoʻāʻo ʻia

760

630

23

140

—

 

 

Ka nui o ka hydrogen diffusion o ka metala i waiho ʻia: ≤4.0mL/100g (ʻano glycerin) 

Nānā X-ray I级: papa I

 

Manaʻo ʻia kēia manawa:

(mm)

Anawaena o ke koʻokoʻo

2.5

3.2

4.0

5.0

(A)

Au Kuʻihao

60 ~ 100

100 ~ 140

140 ~ 190

190 ~ 250

 

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma 350 ~ 380 ℃ ma mua o ka hana kuʻihao;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka unahi ʻaila, ka wai, a me nā mea haumia ma nā ʻāpana wili ma mua o ka wili ʻana;

3. E hoʻohana i ka hana arc pōkole i ka wā e kuʻi ai. He kūpono ke ala kuʻi haiki.

 