J607 (AWS E9015-D1) Haʻahaʻa Alloy Steel Weld Electrodes High-Strength Steel Electrode

ʻO ka wehewehe pōkole:

ʻO J607 (AWS E9015-D1) he mea hao hao kiʻekiʻe kiʻekiʻe me ka haʻahaʻa-hydrogen sodium coating.


Huahana Huahana

Huahana Huahana

Haʻahaʻa Alloy SteelwiliwiliElectrode

J607                                       

GB/T E6015-D1

AWS E9015-D1 

 

ʻO ka wehewehe: ʻO J607 kahi haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa ikaika ikaika electrode me ka haʻahaʻa-hydrogen sodium coating.E hoʻohana i ka DCEP (direct current electrode positive), a hiki ke wili ʻia ma nā kūlana a pau.

Noi: Hoʻohana ʻia no ka wiliwili ʻana i ke kila kalapona liʻiliʻi a me nā hale kila kiʻekiʻe o ka ikaika like, e like me Q420, etc.

 

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

Hua ikaika

Mpa

ʻO ka lōʻihi

%

Waiwai hopena (J)

-30 ℃

Hōʻoiaʻiʻo

≥590

≥490

≥15

≥27

Hoʻāʻo ʻia

620 ~ 680

≥500

20 ~ 28

≥27

 

Maʻiʻo hydrogen diffusion o ka metala i waiho ʻia: ≤4.0mL/100g (ʻano glycerin) 

X-ray inspection: I ka helu

 

Manaʻo ʻia i kēia manawa:

(mm)

Anawaena lāʻau

2.0

2.5

3.2

4.0

5.0

5.8

(A)

wiliwiliʻO kēia manawa

60 ~ 80

70 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

210 ~ 260

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma 350 ℃ ma mua o ka hana wili;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka aila unahi, ka wai, a me nā haumia ma nā ʻāpana wili ma mua o ka wili ʻana;

3. E hoʻohana i ka hana pōkole i ka wā e wili ai.Pono ke ala wiliwili haiki.