Wehewehe Pōkole:

ʻO J421X (AWS E6013) kahi electrode i uhi ʻia me ka titanium-potassium kiʻekiʻe no nā hana kuʻi kila kalapona.


Nā kikoʻī huahana

Nā Lepili Huahana

Kuʻihao kila kalaponaʻElekoda

J421X                                                      

GB/T E4313

ʻAWS A5.1 E6013

Wehewehe: He electrode i uhi ʻia me ka titanium-potassium kiʻekiʻe ʻo J421X no nā hana wili kila kalapona. Hiki iā ia ke hana ma ke kūlana kū i lalo, a kūpono no ka wili ʻana i nā kūlana āpau me nā hana wili maikaʻi loa, a hiki ke hoʻohana ʻia no AC a me DC. He laumania a maʻemaʻe ka wili ʻana. Paʻa ka ʻāʻī a maʻalahi hoʻi e hahau hou, hiki ke wehe maʻalahi ʻia ka slag.

 Hoʻohana: Pili ia i ka hoʻopili ʻana i ke kila kalapona moku a me ka papa kila galvanized, ʻoi aku hoʻi, hoʻopili i ka hoʻopili ʻana o ka papa lahilahi i kahi kūlana kū i lalo a me ka noi hoʻopili discontinuous.

 

Ka hoʻohuihui kemika o ka metala i hoʻoheheʻe ʻia (%):

C

Mn

Si

S

P

≈0.08

≈0.5

≈0.25

≤0.035

≤0.040

 

Nā ʻano mechanical o ka metala i hoʻoheheʻe ʻia:

Mea hoʻāʻo

Ikaika tensile

Mpa

Ikaika hāʻawi

Mpa

Hoʻolōʻihi

%

Ka waiwai hopena (J)

Mahana Maʻamau.

0℃

Hōʻoiaʻiʻo ʻia

≥420

≥330

≥17

—

—

Ua hoʻāʻo ʻia

460 ~ 540

370 ~ 420

≈25

≈80

≈70

 Nānā X-ray: papa II

 

Manaʻo ʻia kēia manawa:

Anawaena o ke koʻokoʻo

(mm)

2.0

2.5

3.2

4.0

5.0

Au wili

(A)

50 ~ 70

60 ~ 100

80 ~ 150

160 ~ 200

180 ~ 250

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana oʻeleka uila hoʻoheheʻes, nā koʻokoʻo kuʻihao, a me nā mea hoʻopau kuʻihao no nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me ke kila kilaʻeleka uila hoʻoheheʻes, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili hao nickel & cobalt, nā uea wili kila akahai & haʻahaʻa, nā uea wili kila kila ʻole, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili hao nickel & cobalt, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 