TYUE E7018 ʻELECTRODE KILA KALAPONA

Wehewehe Pōkole:

ʻElekoda kila kalapona i uhi ʻia i ka pauka haʻahaʻa ....


Nā kikoʻī huahana

Nā Lepili Huahana

Hoʻokaʻawale ʻana:

AWS A5.1 E7018

ISO 2560-B-E4918A

GB/T 5117 E5018

ʻO nā koʻokoʻo wiliwili ʻo AWS E7018 he electrode kila kalapona hao haʻahaʻa hydrogen potassium. Hoʻonui ka lepo hao i loko o ka uhi i ka helu waiho. Loaʻa iā ia ka hoʻohana maikaʻi loa e hiki ai iā ia ke loaʻa kahi arc paʻa, ka liʻiliʻi o ka spatter, maʻalahi ka wehe ʻana i ka slag a hoʻopili ʻia ma nā kūlana āpau. Loaʻa i ka metala i waiho ʻia nā waiwai mechanical maikaʻi e hāʻawi ana i ka paʻakikī wela haʻahaʻa maikaʻi loa.

Ka hoʻohuihui kemika (%)
Ka Hoʻohui Kemika

C

Mn

Si

S

P

Waiwai Hoʻohiki

≤0.12

≤1.60

≤0.75

≤0.035

≤0.040

Hopena Laulā

0.089

1.2

0.38

0.028

0.04

Nā waiwai mechanical o ka metala i waiho ʻia
Mea Hoʻāʻo

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) -30°C

Waiwai Hoʻohiki

≥490

≥400

≥20

≥27

Hopena Laulā

515

430

32

156

Kuhikuhi au (DC)

Anawaena

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

60 ~ 100

80 ~ 140

110 ~ 210

160 ~ 230

Kūlana Kuʻihao:

PA, PB, PC, PD, PE, PF

Nā memo:
1. Pono e hoʻomehana mua ʻia ka electrode ma ka mahana o 350°C no 1 hola. E hoʻomehana mua i ke koʻokoʻo i ka wā e hoʻohana ʻia ai.
2. Pono e hoʻomaʻemaʻe ʻia nā mea haumia e like me ka ʻōpala, nā ʻaila a me ka makū mai ka ʻāpana hana.
3. Pono ke ʻano pōkole e hana i ka wili. Makemake ʻia ke ala wili haiki.

 

Hoʻolohe:

  1. Tpono e hoʻomaloʻo hou ʻia ka electrode ma 350℃-380℃no 1 hola ma mua o ka hoʻomoʻa ʻana.
  2. TPono e wehe ʻia ke koena, ka ʻaila, ka wai a me nā mea haumia ʻē aʻe o ka wahi i hoʻoheheʻe ʻia ma mua o ka hoʻoheheʻe ʻana.