AWS E7015-A1 Heat-Resistant Steel Electrode R107 Low Hydrogen Welding Rods Stick Electrode

ʻO ka wehewehe pōkole:

ʻO R107 (AWS E7015-A1) he pearlitic heat-resistant steel electrode me ka haʻahaʻa-hydrogen sodium coating i loaʻa ka 0.5% Mo.


Huahana Huahana

Huahana Huahana

Molybdenum a me Chromium Molybdenum Heat Resistant SteelwiliwiliElectrode

R107                                                     

GB/T E5015-A1

AWS A5.5 E7015-A1

ʻO ka wehewehe: R107 he pearlitic heat-resistant steel electrode me ka haʻahaʻa-hydrogen sodium coating i loaʻa ka 0.5% Mo. E hoʻohana i ka DCEP (direct current electrode positive) a hiki ke welded i nā kūlana āpau. .

Hoʻohana: Hoʻohana ʻia ia no ka hoʻopili ʻana i nā paipu paila me ka mahana hana ma lalo o 510 ° C (e like me 15Mo, a me nā mea ʻē aʻe), a hiki ke hoʻohana ʻia no ke kuʻi ʻana i ke kila ikaika kiʻekiʻe.

 

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Si

Mo

S

P

≤0.12

0.50~ 0.90

≤0.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

Hua ikaika

Mpa

ʻO ka lōʻihi

%

Waiwai hopena (J)

Ma'amau Temp.

Hōʻoiaʻiʻo

≥490

≥390

≥22

≥47

 

Maʻiʻo hydrogen diffusion o ka metala i waiho ʻia: ≤6.0mL/100g (ʻano glycerin)

X-ray inspection: I ka helu

 

Manaʻo ʻia i kēia manawa:

Anawaena lāʻau

(mm)

2.0

2.5

3.2

4.0

5.0

wiliwiliʻO kēia manawa

(A)

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma 350 ℃ ma mua o ka hana wili;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila unahi, ka wai, a me nā haumia ma nā ʻāpana wili ma mua o ka wili ʻana.