AWS E9015-B9 Paʻa Paʻa Paʻa Arc Welding Rod Stick Welding Electrodes Filler Metal

ʻO ka wehewehe pōkole:

ʻO R717 (AWS E9015-B9) he electrode kila me ka haʻahaʻa-hydrogen sodium i loaʻa iā 9% Cr - 1% Mo-V-Nb.


Huahana Huahana

Huahana Huahana

Molybdenum a me Chromium Molybdenum Heat Resistant Steel Weld Electrode

R717                                                     

AWS A5.5 E9015-B9

ʻO ka wehewehe ʻana: R717 he electrode kila me ka haʻahaʻa-hydrogen sodium coating i loaʻa ka 9% Cr - 1% Mo-V-Nb.E hoʻohana i ka DCEP (direct current electrode positive) a hiki ke wili ʻia ma nā kūlana āpau.Ma muli o ka hoʻohui ʻana o kahi liʻiliʻi o Nb a me V, ʻoi aku ka maikaʻi o ka metala i hoʻopaʻa ʻia.

 

Hoʻohana: Hoʻohana ʻia ia no ka hoʻopili ʻana i nā paipu superheated a me nā poʻo o ka wela wela a me nā paila kiʻekiʻe, e like me A213-T91/A335-P1 (T/P91), A387Cr, 91 a me nā hale kila pale wela.

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Si

Cr

Mo

V

Ni

0.08 ~ 0.13

≤1.20

≤0.30

8.0 ~ 10.5

0.85 ~ 1.20

0.15 ~ 0.30

≤0.80

Nb

Cu

Al

N

S

P

 

0.02 ~ 0.10

≤0.25

≤0.04

0.02 ~ 0.07

≤0.01

≤0.01

 

Hoolaha: Mn+Ni<1.5%

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

Hua ikaika

Mpa

ʻO ka lōʻihi

%

Hōʻoiaʻiʻo

≥620

≥530

≥17

 

Manaʻo ʻia i kēia manawa:

Anawaena lāʻau

(mm)

2.5

3.2

4.0

5.0

Ke au wiliwili

(A)

60 ~ 90

90 ~ 120

130 ~ 170

170 ~ 210

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma 350 ℃ ma mua o ka hana wili;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila unahi, ka wai, a me nā haumia ma nā ʻāpana wili ma mua o ka wili ʻana.

3. E hoʻomaʻamaʻa mua i ka ʻāpana weld ma 200 ~ 260 ° C ma mua o ke kuʻi ʻana, a mālama i ka mahana interpass kūpono;

4. Hoʻomaha mālie i ka 80 ~ 100 ° C no nā hola 2 ma hope o ke kuʻiʻana;inā ʻaʻole hiki ke hana ʻia ka hoʻomaʻamaʻa wela i ka hikiwawe, hiki ke hana ʻia ka hana dehydrogenation ma 350°CX 2h.

 