Wehewehe Pōkole:

ʻO ka electrode kumu e waiho ana i kahi kila manganese austenitic, ka mea e hoʻopaʻakikī ʻia e ka deformation anu, pili i nā kila o ke ʻano like a ma nā ʻāpana i hoʻopilikia ʻia e nā hopena koʻikoʻi a me ka abrasion waena.


Nā kikoʻī huahana

Nā Lepili Huahana

ʻElektrode Laʻau Kuʻi PaʻakikīRODO P

RODO PARA RECUBRIMIENTO PALU

ʻAno Helu: D256 (B – 80)

Ka Nānā ʻana i ka Metala i Waiho ʻia (Nā waiwai maʻamau)

C

1.2%

Mn

13.0%

Si

0.5%

Ni

3.0%

 

Nā ʻano:

ʻO ka electrode kumu e waiho ana i kahi kila manganese austenitic, ka mea e paʻakikī ai ma o ka deformation anu, e pili ana i nā kila o ka haku mele like a ma nā ʻāpana i kau ʻia i nā hopena koʻikoʻi a me ka abrasion waena. He kūpono ia no ka hoʻōla ʻana, ka uhi ʻana a me ka hoʻoponopono ʻana i nā ʻāpana kila Mn austenitic, nā ʻāpana a me nā ʻāpana o nā mīkini kaumaha.

 

Nā Waiwai Mekanika:Paʻakikī 200-250 HB BRINELL i ka waiho ʻana, 300-400 HB Brinell

ma hope o ka paʻakikī ʻana o ka hana anu.

 

Nā Kūlana Kuʻihao:Palahalaha, Lauoho, Luna, Kū i luna.

 

Keia manawa a me ka Polarity:

No ke au uila a i ʻole ke au uila pololei

ka electrode i ka pou maikaʻi

ʻoe mm

ʻoe i loko

Amperage

3.20

1/8

110-130

4.00

5/32

140-160

5.00

2/16

180-230

 

Nā Hana: • No ka hoʻopiha ʻana i nā kila manganese.

• Ke kūkulu hou ʻana i nā niho ʻeli a me nā bākeke.

• Nā keʻa a me nā puʻuwai o nā alahao.

• Nā wili mineral a me nā hāmare.

• Ma ke kuʻi ʻana, piʻi kona paʻakikī i 350 – 400 HB.

• I ke kūkulu hou ʻana a i ʻole ka uhi hou ʻana, e hoʻohana iā AG AR-91 ma ke ʻano he kumu.

• Ma nā mahana ma luna o 300 OC, nā kila Mn

Hoʻomaka lākou e nalowale i ka paʻakikī. Paipai ʻia nā kaula

lele ʻia, ke anawaena haʻahaʻa loa a me ka amperage hiki.

 

 

LOA: 350mm.

KAONA NO KA PAHU: 20 kg/44 lbs.

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. i ka makahiki 2000. Ua hana mākou i ka hana ʻana oʻeleka uila hoʻoheheʻes, nā koʻokoʻo wili, a me nā mea hoʻopau kuʻihao no nā makahiki he 20 a ʻoi.

ʻO kā mākou huahana nui e komo pū me ke kila kilaʻeleka uila hoʻoheheʻes, nā electrodes wili kila kalapona, nā electrodes wili hao haʻahaʻa, nā electrodes wili ʻili, nā electrodes wili hao nickel & cobalt, nā uea wili kila akahai & haʻahaʻa, nā uea wili kila kila ʻole, nā uea wili flux cored gas-shielded, nā uea wili alumini, ka wili arc submerged. nā uea, nā uea wili hao nickel & cobalt, nā uea wili keleawe, nā uea wili TIG & MIG, nā electrodes tungsten, nā electrodes gouging kalapona, a me nā mea pono wili a me nā mea hoʻopau ʻē aʻe.

 

 

 

 