Wehewehe Pōkole:

ʻO E410NiMo-15 kahi electrode wili kila kila martensitic me ka uhi sodium haʻahaʻa-hauwai 11.0-12.5% ​​Cr, 4.0-5.0 Ni, a me 0.40-0.70% Mo.


Nā kikoʻī huahana

Nā Lepili Huahana

Kūlana Kūlike

GB/T 983-2012 E410NiMo-15

ʻO AWS A5.4M-2012 E410NiMo-15

Mea like:1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM,UNS S41500

Wehewehena

ʻO E410NiMo-15 kahi electrode wili kila kila martensitic me ka uhi sodium haʻahaʻa-hydrogen, nona ka 11.0-12.5% ​​Cr, 4.0-5.0% Ni, a me 0.40-0.70% Mo. He kūpono ia no ka wili hao pale āpau (SMAW) me ke arc paʻa, ka liʻiliʻi o ka spatter, a me ka hiki ke wehe ʻia ka slag maikaʻi loa. Hāʻawi ka metala i waiho ʻia i ka ikaika kiʻekiʻe, ke kūpaʻa maikaʻi i ka corrosion, a me ke kūpaʻa i ka haki ʻana. Manaʻo ʻia ka hoʻomehana mua ʻana no nā ʻāpana hana mānoanoa, a pono ka mālama wela ma hope o ka wili ʻana (PWHT) ma 580 ~ 620 ℃ (1-2 mau hola, hoʻoluʻu ea, AC).

Noi

Kūpono no ka hoʻoheheʻe ʻana i ke kila kila ASTM CA6NM, nā kila moʻo 13% Cr-4% Ni (e laʻa, Cr13Ni4Mo, Cr13Ni5Mo), a me nā kila kila martensitic like. ʻO nā noi maʻamau e pili ana i ka hoʻoponopono ʻana i ka hoʻoheheʻe ʻana o nā mea holo turbine hydropower, nā kino valve, nā pipeline kiʻekiʻe, a me ka ʻili ʻana o nā ʻāpana i hoʻopaʻa ʻia e ka cavitation. Hoʻohana pū ʻia no ka hoʻoponopono ʻana i nā ʻāpana pale ʻaʻahu e like me nā ʻōwili crusher a me nā pahu pamu.

Ka Hoʻohui Kemika o ka Metala Weld (%)

ʻElemene C Mn Si P S Cr Ni Mo Cu
Koi ≤0.06 ≤1.0 ≤0.90 ≤0.04 ≤0.03 11.0-12.5 4.0-5.0 0.40-0.70 ≤0.75
Hopena Hoʻāʻo 0.029 0.7 0.32 0.028 0.01 12.26 4.50 0.55 0.01

Nā Waiwai Mekanika o ka Metal i Waiho ʻia

Inoa Hoʻāʻo Ikaika Tensile (Mpa) Hoʻolōʻihi% X-Ray Hoʻāʻo hopena,(+20 ℃)J Paʻakikī HB Hydrogen Hoʻolaha (ml/100g)
Nā Koi ≥760 ≥15 Papa I – – ≤5
Hopena Hoʻāʻo 845 19 Papa I 60-90 250-310 ≤5

Nā Palena Kuʻi i Manaʻo ʻia

Puna Mana: Mālama DC (DC-)

Manaʻo ʻia kēia manawa

Ke Anawaena o ke Koʻokoʻo (mm) 3.2 4.0 5.0
Au Kuʻihao (A) 80-120 120-160 150-190

Hoʻolaha:

1. E hoʻomoʻa i ka electrode ma 300 ℃ no hoʻokahi hola ma mua o ka hoʻohana ʻana e wehe i ka makū.
2. E hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila, a me ka makū mai ka ʻili metala kumu; e hoʻohana i ka hana arc pōkole no nā momi weld haiki.
3. Pono e hana koke ʻia ka PWHT ma hope o ka hoʻoheheʻe ʻana e pale aku i ka embrittlement.