ʻO nā koʻokoʻo wiliwili kila kila AWS A5.4 E310H-16 mea hoʻolako uila uila maikaʻi loa.

ʻO ka wehewehe pōkole:

ʻO A432 (AWS A5.4 E310H-16) he 3Cr26Ni21 me ka hoʻoheheʻe ʻia me ka titanium-calcium coating.


Huahana Huahana

Huahana Huahana

Kuʻihao KuʻihaoElectrode

A432                                 

GB/T E310H-16

AWS A5.4 E310H-16

ʻO ka wehewehe ʻana: ʻO A432 kahi 3Cr26Ni21 me ka hoʻoheheʻe ʻana i ka titanium-calcium.Hiki ke hoʻohana ʻia no ka AC a me DC me ka hana maikaʻi loa.ʻO ka metala i waiho ʻia he ikaika kolo kiʻekiʻe, maikaʻi ka hui pū ʻana, a me ka haʻahaʻa haʻahaʻa haʻahaʻa.

Noi: Hoʻohana kūikawā ia no ka wiliwili ʻana i ke kila wela HK40.

 

ʻO ka hui kemika o ka weld metala(%):

C

Cr

Ni

Mo

Mn

Si

Cu

S

P

0.35 ~ 0.45

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

1.0 ~ 2.5

≤0.75

≤0.75

≤0.030

≤0.030

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

 

Ka ikaika tensile

Mpa

ʻO ka lōʻihi

%

Hōʻoiaʻiʻo

≥620

≥10

 

Manaʻo ʻia i kēia manawa:

Anawaena lāʻau

(mm)

3.2

4.0

5.0

Ke au wiliwili

(A)

80 ~ 110

110 ~ 160

160 ~ 200

 

Hoʻolaha:

  1. Pono e kālua ʻia ka electrode no 1 hola ma kahi o 150 ℃ ma mua o ka hana wili;
  2. No ka mea he pāpaʻu ka hohonu o ke komo ʻana i ka wā hoʻoheheʻe AC, pono e hoʻohana ʻia ka mana DC e like me ka hiki ke loaʻa ka hohonu hohonu.a ʻaʻole pono e nui ke au e pale aku i ka ʻulaʻula o ke koʻokoʻo kuʻi.

 

 

Ua hoʻokumu ʻia ʻo Wenzhou Tianyu Electronic Co., Ltd. ma 2000. Ua hana mākou i ka hana ʻana owiliwili uilas, lāʻau wiliwili, awiliwili mea hoopauno nā makahiki ʻoi aku ma mua o 20.

ʻO kā mākou huahana nui he kila kilawiliwili uilas, kalapona kila kuʻihao electrodes, haʻahaʻa wili kuʻihao electrodes, surfacing kuʻihao electrodes, nickel & cobalt kuʻihao kuʻihao electrodes, mild kila & haʻahaʻa wili kuʻihao uea, kuhiliʻole kila kuʻihao uea, kinoea-pale flux cored uea, aluminika kuʻihao uwea, submerged arc kuʻihao. .uea, nickel & cobalt alloy uea, keleawe wiliwili uea, TIG & MIG wiliwili uea, tungsten electrodes, carbon gouging electrodes, a me na mea wiliwili 'ē aʻe a me nā mea hoʻohana.

 