AWS E9015-G Haʻahaʻa Alloy Steel wiliwili haʻahaʻa haʻahaʻa hydrogen wiliwili Electrodes J607CrNiMo

ʻO ka wehewehe pōkole:

ʻO J607CrNiMo (AWS E9015-G) kahi mea hao hao hao haʻahaʻa me ka haʻahaʻa hydrogen sodium coating.


Huahana Huahana

Huahana Huahana

Haʻahaʻa Alloy Steel Weld Electrode

J607CrNiMo                                       

GB/T E6015-G

AWS E9015-G

 

Hōʻike: J607CrNiMo he haʻahaʻa haʻahaʻa kila electrode me ka haʻahaʻa hydrogen sodium coating.E hoʻohana i ka DCEP (direct current electrode positive), a hiki ke wili ʻia ma nā kūlana āpau me ka hana pōkole pōkole.ʻO ke koʻokoʻo kuʻihao he hohonu ke komo ʻana, emi ka spatter a me ka hana hana maikaʻi.He maikaʻi ka plasticity i waiho ʻia me ka metala, haʻahaʻa haʻahaʻa haʻahaʻa haʻahaʻa a me ka pale ʻana.

Hoʻohana: Hoʻohana ʻia ia no ka hoʻopaʻa ʻana i nā paipu wai ma lalo o 350 °C i nā kikowaena mana a me nā mea hao pahu kaomi o nā māka ikaika kūpono.Loaʻa iā ia kahi pāʻani maikaʻi me ke kila WB36CN1 (HD15Ni1MnMoNbCu) kūloko, a he kūpono hoʻi no ka hoʻopili ʻana i ke kila WB3 (15NiCuMoNb5).

 

ʻO ka hui kemika o ka weld metala(%):

C

Mn

Si

Cr

Ni

Mo

S

P

≤0.10

1.00 ~ 1.60

≤0.50

0.14 ~ 0.35

0.60 ~ 1.20

0.15 ~ 0.50

≤0.015

≤0.015

 

Nā waiwai mīkini o ka weld metala:

Mea ho'āʻo

Ka ikaika tensile

Mpa

Hua ikaika

Mpa

ʻO ka lōʻihi

%

Waiwai hopena (J)

-30 ℃

Hōʻoiaʻiʻo

620 ~ 720

≥500

≥20

≥47

 

Maʻiʻo hydrogen diffusion o ka metala i waiho ʻia: ≤5.0mL/100g (mercury a i ʻole gas chromatography method)

X-ray inspection: I ka helu

 

Manaʻo ʻia i kēia manawa:

(mm)

Anawaena lāʻau

3.2

4.0

5.0

(A)

Ke au wiliwili

100 ~ 140

140 ~ 18

190 ~ 230

 

Hoʻolaha:

1. Pono e hoʻomoʻa ʻia ka electrode no 1 hola ma kahi o 350 ℃ ma mua o ka hana wili;

2. He mea nui e hoʻomaʻemaʻe i ka ʻōpala, ka ʻaila unahi, ka wai, a me nā haumia ma nā ʻāpana wili ma mua o ka wili ʻana.