ʻELECTRODE KILA KĪNĀ E316L-16

Wehewehe Pōkole:

E316L-16 Kuʻihao ʻana o ke kalapona haʻahaʻa loa 18% Cr-12% Ni-2% Mo (kila kila 316L)


Nā kikoʻī huahana

Nā Lepili Huahana

Nā Koko Hana Kuʻihao Kila Kila ʻO AWS A5.4 E316L-16

AWS: SFA 5.4 E316L-16

ʻO: 5206 E19.12.2.LR16

EN ISO CODE: 3581-AE 19 12 3 LR 3 2

Nā ʻano ma ka hoʻohana ʻana:

ʻO E316L-16 kahi electrode ʻano lime-titania i hāʻawi ʻia me ka hoʻohana maikaʻi a me ka hiki ke hoʻopili ʻia.

Ma muli o ke ʻano austenite o ka metala i hoʻoheheʻe ʻia me ka nui kūpono o ka ferrite, maikaʻi ke kūʻē ʻana i ka māwae. Loaʻa iā ia ke kūʻē maikaʻi loa i ka corrosion intercrystalline i ke kūlana as-welded ʻoiai ʻoi aku ka liʻiliʻi o ka nui o ke kalapona a ʻoi aku ka maikaʻi o ke kūʻē ʻana i ka corrosion intergranular ma mua o ko E316L-16 a loaʻa iā ia ka Mo. Maikaʻi nō hoʻi ke kūʻē ʻana i ka wela.

He kiʻekiʻe ke kūpaʻa ʻana o E316L-16 i ka makū a me ka pale ʻana i ka porosity maikaʻi.

KA HOʻOHUI KEMIKA O NĀ MEA WELD A PAU (%)

ʻElemene

C

Mn

Si

Cr

Ni

Mo

S

P

Cu

Pakeneka

≤0.04

0.50-2.50

≤0.90

17-22

11-14

2.0-3.0

≤0.030

≤0.04

≤0.75

Nā Waiwai Mīkini o nā Metala Welded āpau

UTS

Hoʻolōʻihi

(MPa)

(L= 5d)%

545

40

ʻIkepili o kēia manawa a me ka hoʻopili ʻana: AC / DC(+)

Nui (mm)

5×350

4×350

3.15×350

2.5×350

Ka Pae o kēia Manawa (Amps)

150-180

110-140

80-100

60-80

Kaumaha / Pahu (kgs)

2.5

2.5

2.5

2.5

Ka Makaʻala

1. E hoʻohana i ke arc pōkole a me ke kaula stringer e kāohi i ka hoʻokomo ʻana o ka wela.

2. E hōʻoia i ka maloʻo o nā electrodes. E hoʻomaloʻo hou i nā electrodes ma 250-300°C no hoʻokahi hola.

Nā memo no ka hoʻohana ʻana:

Pono ka laulā o ka ulana ʻana i loko o ʻelua a me ka hapa manawa o ke anawaena o ka electrode.

E wehe i nā mea lepo e like me ka ʻaila a me ka lepo mai loko mai o ke awāwa.

E hoʻomaloʻo i nā electrodes ma 350 (662) no 60 mau minuke ma mua o ka hoʻohana ʻana.